8th Jul 2022, 07:51 PM #16Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,561
-
9th Jul 2022, 04:44 AM #17
Hi Michael,
If they are cylinder head studs that could be correct, though 13 X 1 is almost a gas thread size.Best Regards:
Baron J.
-
9th Jul 2022, 07:53 AM #18Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,561
It's just a thought John. The reason I raise it is that the threaded ends will have to go into either a nut or a tapped hole, but if they are non-standard, then how was that matching thread created as taps would not be readily available either?
The item could be a cylinder stud, but typically threads into a casting have a coarser pitch, so I would have expected something like a (more common) M12x1.75. I would also expect a longer length of thread than 10mm either end. While tinkering away in the shed I did find a thread a few weeks back that was x/32"; I think it turned out to be a little used BSF size. 12mm is close to 15/32" and 13mm is close to 1/2" so that set me thinking...
It would be really annoying for Ross to get all set up to cut these threads and then discover that the part he has made does not quite fit. Better to check now.
Michael
-
9th Jul 2022, 11:33 AM #19I break stuff...
- Join Date
- Aug 2010
- Location
- Toorloo Arm, VIC
- Age
- 39
- Posts
- 1,295
12x1.5 is by absolutely no means an uncommon thread in my experience, got plenty of bolts and other bits around here which are that thread, along with taps to suit. Googling "12x1.5 tap" gives pages of results, the first from Sutton.
Many of the common thread tables only list metric 'coarse' threads, and omit other quite common threads in what is sometimes referred to as metric 'fine' (a constant source of headache to me). Even when they DO list a fine pitch, they only list one, and my experience suggests that there is often an even finer pitch in common use than 'fine'. If you play with European vehicles, (definitely Italian ones), you'll very quickly learn of the existence of 8x1.0, 10x1.0, 10x1.25, 12x1.25, 12x1.5, as a LOT of bolts are these threads - and sometimes go into aluminium castings to boot. I've wasted hours of my life trying to remove a stud from Alfa 156/147 gearboxes in order to remove the gearbox and replace the clutch - from memory the thread on that bastard of a thing was 18x1.25, or possibly by 1.5. Up the back of the motor, getting an eighth of a turn at a time at best, and the thread was always thoroughly grown to the aluminium. No matter how much Inox and back and forth you did, it was luck of the draw whether the thread in the casting would come out with it or not. Not uncommon for it to take over an hour to get that one stud out.
The banjo bolts for turbo oil supply pipes can be any of 10x1.0, 10x1.25 or 10x1.5 - all common on various late model vehicles.
You also come across some truly oddball stuff - Alfetta GTV6 lower sump bolts are 7x1.0 from memory, for some absolutely unknown reason given the abundance of both 8x1.25 and 8x1.0 bolts elsewhere on the vehicles. Think I've encountered both 9mm and 11mm fine pitch bolts before too. So while 13x1.0 I would definitely personally class as pretty uncommon, I'm sure it exists and has been used somewhere. Indeed a quick google for 13x1.0 taps does return a couple of results...
All depends on the machine/equipment, the particular location of the thread and its country of origin. Generally continental European and Asian stuff I'd be pretty confident it is metric, but for older British, American and Australia I'd be looking more for a suitable imperial thread. Newer British or Australian, most likely metric again. Anything to do with hydraulics or possible pipe threads - could be anything under the sun.
Around here, 12x1.5 normally wouldn't raise an eyebrow unless I found it on some of the ancient Australian or British crap I have laying around here. (It's happened before, usually someones stripped a bolt and rethreaded, but not always). 13x1.0, highly dependent on where exactly I found it as to whether I'd believe it to be metric or be rather suspect of it being some form of imperial thread.
-
9th Jul 2022, 11:52 AM #20Most Valued Member
- Join Date
- Nov 2007
- Location
- melbourne australia
- Posts
- 3,228
This is the solution IMO. Dies are available in both sizes. Gotta be easier than trying to get an imperial lathe to turn metric threads when you don't have the appropriate change gears.
M12x1.5 die (select from drop-down menu):
https://sydneytools.com.au/product/d...BoCprsQAvD_BwE
M13x1 die:
https://www.ebay.com.au/itm/32450881...BoCcJUQAvD_BwEChris
-
11th Jul 2022, 10:41 AM #21Intermediate Member
- Join Date
- Apr 2009
- Location
- Perth AU
- Posts
- 36
Thank you Michael you have pointed out an error in my original post.
The smaller thread is actually M12x1.25 and this has been confirmed with a standard nut.
The larger thread has been confirmed as M13x1.0 by an ex machinist who now sells engineering hardware. He did say that thread was not very common but definitely part of a "standard". An engineer once said to me "The good thing about standards is there are so many to choose from"
To put this into a better picture for you the part I am making is to replace a stand off for the trucks on a pair of roller skates. The original was made of aluminium and he kept breaking it so we agreed to try it in BMS. The large end screws into the sole plate on the base of the skate.
I will look at your links Jack620 and consider the options.
The second part of my journey is to be able to cut metric threads in the future too. So, while I could buy the dies, if I don't invest in the change gears I am limiting my ability in that respect. I already have a reasonable set of metric taps and dies but if I can use the lathe the world is my oyster.
We have a Myford at work with a full set of metric change gears which have never been used so I am looking at using that for this job and will look at Mal's offerings for my lathe.
Cheers,
-
11th Jul 2022, 05:23 PM #22
Hi Ross, Guys,
I too have an Imperial Myford lathe, a S7LB with a quick change gearbox, I don't have any metric gears as such ! But by changing one gear I can cut most metric and BA threads along with some quite strange threads if you get the gearbox settings wrong.
The only gear that is changed is the one immediately following the tumbler gears. I don't recall what number of teeth without going and looking but there is also a couple of charts giving the gear and gearbox settings on the
The home of Model Engineer and Model Engineers' Workshop Magazines web site.
I'm not at home right now, so not able to go and look at mine.Best Regards:
Baron J.
-
12th Jul 2022, 11:04 AM #23Intermediate Member
- Join Date
- Apr 2009
- Location
- Perth AU
- Posts
- 36
Look forward to that information BaronJ
Cheers,
-
16th Jul 2022, 08:52 PM #24
Have a read of this thread
https://www.model-engineer.co.uk/for...?th=140427&p=1
I have both the 33 & 34 tooth gears, I also printed out the gearbox setting charts.
The weather in Scarborough, East Yorkshire, UK was very nice this last weekBest Regards:
Baron J.
-
17th Jul 2022, 01:40 PM #25Intermediate Member
- Join Date
- Apr 2009
- Location
- Perth AU
- Posts
- 36
Very interesting BaronJ but the Myford gear set is a different beast to the Hercus one so not sure that solution would work straight up.
Have asked a friend to 3D print a set for me so waiting on that as a possible option.
Cheers,
-
17th Jul 2022, 07:01 PM #26
Hi Ross,
I'm sure that I have seen something similar for the "Southbend" and "Hercus" lathes where a gear was changed and the gearbox was adjusted to get various threads. But yes it would depend upon the gear ratios.Best Regards:
Baron J.
-
24th Jul 2022, 04:31 PM #27Intermediate Member
- Join Date
- Apr 2009
- Location
- Perth AU
- Posts
- 36
Well I finally did figure out what that gear set was intended to be used for. They are the gears for the gear hobber which goes in the mill attachment.
To add to the original list I also have 80, 30 and one or two others as well.
I cannot imagine how many ratio options that many gears selections would give but if I ever need to cut a gear at least I know I can.
Cheers,
Gear Hobber.jpg
-
25th Jul 2022, 07:58 PM #28Golden Member
- Join Date
- Oct 2008
- Location
- Cairns, Q
- Posts
- 666
Hi Michael,
FWIW 5/32x32TPI, (5/32W) was a very common thread until quite recently. It was frequently used on drawer pull knobs, and, I think, in some 240V fittings. If my memory is correct (it's been a long time), but I think it was also the thread in the spoke nipples on early twenties Austin 7 wheel spokes.
Frank.
-
27th Jul 2022, 08:07 PM #29australian metalworking hobbyist
- Join Date
- Jan 2009
- Location
- Holbrook, NSW
- Age
- 73
- Posts
- 490
calcs
There are lots of combinations of gears that will let you cut reasonable threads.
These are the two Hercus used for cutting metric threads, that can be used on a 9A lathe with a standard imperial gearbox.
imp-met.jpg
-
3rd Dec 2022, 12:01 AM #30human termite
- Join Date
- Jul 2007
- Location
- sandstone point queensland
- Age
- 69
- Posts
- 182
metric thread cutting
this may help
............bob
Similar Threads
-
Metric threading on Imperial 9"AR Hercus
By auscab in forum THE HERCUS AREAReplies: 9Last Post: 9th May 2021, 11:22 AM -
Hercus 260/9" B and C inch to metric threading chart
By allterrain50 in forum THE HERCUS AREAReplies: 0Last Post: 29th May 2017, 04:22 PM -
Imperial Threading on Metric Leadscrew
By Jenova in forum METALWORK GENERALReplies: 29Last Post: 15th Apr 2017, 11:09 AM -
Hercus 260 Metric - Help with Single Point Threading
By ventureoverland in forum THE HERCUS AREAReplies: 3Last Post: 19th Sep 2014, 11:48 PM -
Metric threading on an imperial lathe
By Vernonv in forum METALWORK GENERALReplies: 9Last Post: 25th Oct 2010, 07:58 AM