Setup for a tailstock turret head
Anorak Bob has very kindly given me a small MT2 tailstock tool turret with 6, 5/8"sockets for tools.
I never really had the need to use it until a recent project where it would have been very handy so its spurred me on to get it up and running.
I thought about setting it up with some (at least 3?) cheap ER16 chucks as I already a set of ER16 collets.
Alternatives are
1) Purchase ER16 chucks with 5/8" shanks - cheapest I can find are from the US @ $80 ea (half is shipping). Not likely! CTC has them for about $20 + shipping but they're out of stick
2) purchase ER16 chucks with 16mm shanks from Aliexpress or EBay for about $12 and turn the 16mm down to 5/87"
3) ER16 chucks with no shank for just $3 on Aliexpress, just a 10 MM socket and grub screw in the back of the chuck. Then turn up some 10mm to 5/8" adapters?
I figured I could one each of 2) and 3) just to see what they are like.
ER16 seems about right the right weight for the Hercus and the turret, but I would also consider a couple of ER20 or 25 chucks, but I would have to buy collet sets.
What do you reckon?
-
24th Apr 2022, 05:45 PM #2
Hi Bob,
I would forget about turning ER collet chuck shanks down, They are as hard as hell frozen over ! You would get away with grinding them down, but I think 0.125 mm (15 thou) might be a lot to grind off.Best Regards:
Baron J.
-
24th Apr 2022, 07:27 PM #3Diamond Member
- Join Date
- Aug 2019
- Location
- Revesby - Sydney Australia
- Age
- 57
- Posts
- 1,195
Bob, if you are game to do some careful machining of the taper (and maybe flame harden the surface later), you could make your own?
Option 3 would certainly be cheapest.
My first thought would be that they would not run true, but then I remembered these are just a tailstock, and the turret location would probably be more of an issue than the 10mm->5/8" adapter concentricity?
Option 2 is possible. As John says, they will be hardened, but throw a CBN tip in, and you can get there.
Note, after some intense searching (i.e. luck), found some on Amazon US for about $47AUD:
https://www.amazon.com/Extension-Str...=1XB8PT99L8OLX
Probably overkill for a free turret, though
-
24th Apr 2022, 08:15 PM #4Member: Blue and white apron brigade
- Join Date
- Feb 2006
- Location
- Perth
- Posts
- 7,189
Thanks for the replies
I already have two cheap ER16 chucks, one with a solid 12mm diameter x (originally) 100mm long, straight shank that I parted with no probs using a HSS parting blade down to about half that length. The other is 150mm long with a hollow shank.
I never thought to test them but testing with my Tsubosan hardness files shows the solid one can be scratched by the HRC 55 but not the 50, The hollow one can be scratched by the 50 but not the 45 so they cant be that hard.
The sockets in the turret aren't tapered they're straight and there's a locking grub screws for each socket.
Turret1.JPG
Option 3 would certainly be cheapest.
My first thought would be that they would not run true, but then I remembered these are just a tailstock, and the turret location would probably be more of an issue than the 10mm->5/8" adapter concentricity?
Option 2 is possible. As John says, they will be hardened, but throw a CBN tip in, and you can get there.
Note, after some intense searching (i.e. luck), found some on Amazon US for about $47AUD:
https://www.amazon.com/Extension-Str...=1XB8PT99L8OLX
Probably overkill for a free turret, though
-
24th Apr 2022, 08:56 PM #5Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,561
You can't take the mounting bores out to 16mm, so you can use the cheaper collets?
Michael
-
24th Apr 2022, 09:39 PM #6Member: Blue and white apron brigade
- Join Date
- Feb 2006
- Location
- Perth
- Posts
- 7,189
-
24th Apr 2022, 10:03 PM #7Diamond Member
- Join Date
- Aug 2019
- Location
- Revesby - Sydney Australia
- Age
- 57
- Posts
- 1,195
Originally Posted by nigelpearson
I meant the ER collet's taper. Machining the whole ER chuck!
Take 25mm round 4140 stock, drill and bore about 20mm deep at 11mm diameter, then taper out at 8° 'till it is 17mm at the face, then machine the thread on the outside for the ER collet nut. Once you have done those precision steps, machining the back to 5/8" is fairly easy?
-
24th Apr 2022, 10:42 PM #8Member: Blue and white apron brigade
- Join Date
- Feb 2006
- Location
- Perth
- Posts
- 7,189
-
28th Apr 2022, 11:51 AM #9.
- Join Date
- Nov 2008
- Location
- Perth WA
- Age
- 71
- Posts
- 6,459
Bob,
Another option might be to purchase a 10 or 12mm straight shanked ER16A chuck and make a split 5/8" sleeve to suit. https://www.ebay.com/itm/16266120727...oAAOxydyxSPbdb
I have purchased some unrealistically cheap AliExpress tooling and it has gone straight into the bin. You could be lucky!
Back when shipping was affordable from the States I purchased a few drill chucks for use in the Enco turret. They were screw mount chucks and I simply made some 5/8" shanks threaded 1/2"UNF to suit. There may be some cheap Chinese chucks available that offer reasonable accuracy and could be an alternative to collet chucks.
1.jpg 2.jpg
Something else that might be worth considering is making some split bushes to suit particular tooling such as centre drills and countersinks. They don't even have to be split, tooling could be retained with a grub screw.
And here are some Hardinge 5/8" reduction bushes or sleeves as an example. And one being used to hold a boring bar in a Hardinge slide.
IMG_20200315_100950273 (1).jpg IMG_20200315_101521351.jpg
Bob.
-
28th Apr 2022, 01:07 PM #10Member: Blue and white apron brigade
- Join Date
- Feb 2006
- Location
- Perth
- Posts
- 7,189
Thanks Bob, some interesting possibilities there. I think I’m going to wait for CTC to get the 5/8” shanked ER16 back in stock although it might take some time. What with Covid and associated supply chain issues. Only yesterday I ordered some sealable plastic bags for 3D printer filament storage and got a reply saying “ We are in Shanghai and totally locked down and cannot get any goods in or out etc and do you want a refund”
All of the CTC stuff I’ve bought so far has been reasonable quality.
-
28th Apr 2022, 01:23 PM #11.
- Join Date
- Nov 2008
- Location
- Perth WA
- Age
- 71
- Posts
- 6,459
Bob,
There is something else that should probably be investigated before you hit the 'buy it now' button. The alignment of those 5/8" bores.
Probably worth turning up a test bar and running an indicator along the bar with it mounted in the turret. It you find things out of whack it wouldn't be a bad idea to rebore the holes out to 16mm. I can lend you a nice boring head if you don't have one.
Bob.
-
28th Apr 2022, 01:45 PM #12Member: Blue and white apron brigade
- Join Date
- Feb 2006
- Location
- Perth
- Posts
- 7,189
Similar Threads
-
Need setup for tailstock issue
By phaser in forum METALWORK GENERALReplies: 17Last Post: 18th Jan 2021, 01:30 PM -
About a low cost Tailstock Turret...
By cba_melbourne in forum METALWORK GENERALReplies: 7Last Post: 13th Jan 2015, 07:49 AM -
Tailstock Turret
By Anorak Bob in forum METALWORK GENERALReplies: 8Last Post: 2nd Jan 2015, 01:42 PM -
Tailstock Turret
By Big Shed in forum METALWORK GENERALReplies: 36Last Post: 9th Jul 2009, 07:40 PM -
Can I use a Boring Head in the Tailstock
By Retromilling in forum METALWORK GENERALReplies: 17Last Post: 29th Jun 2009, 04:30 PM