Thanks: 0
Results 1 to 4 of 4
Thread: Butchered topslide Hercus 9"
-
6th Nov 2021, 05:31 PM #1New Member
- Join Date
- May 2009
- Location
- Sydney
- Posts
- 8
Butchered topslide Hercus 9"
I've had this 9" model C for 38 years and have only ever done light work with it. The graunched top slide is as I bought it and I assume it met its fate in a schoolroom workshop when chuck met top slide and chuck won.
I now find that as I use the parting tool more I am getting movement between toolholder and top slide and I am breaking parting tips during light or heavy use. My presumption is the loss of load bearing area on the top slide is contributing to the tool holder instability. I also understand parting off can be a dark art
Has anyone had one of these slides satisfactorily repaired by welding/brazing or any other method, or is it a replacement from somewhere
Advice would be appreciated
AlanMcl
-
7th Nov 2021, 09:26 PM #2Diamond Member
- Join Date
- Aug 2019
- Location
- Revesby - Sydney Australia
- Age
- 57
- Posts
- 1,196
Hi Alan.
I recognise that sort of damage. Here is my ex-school compound slide:
IMG_1368.jpg IMG_0084.jpg
I don't think your slide's damage will impact cutting or parting very much.
1) If you have the standard "lantern" toolpost, its clamping area is a disc that is well away from the damaged edge:
Screen Shot 2021-11-07 at 8.39.08 pm.jpg
2) If you have a Hercus square 4way toolpost, or a newer QCTP (like Swiss Multi*), it is a larger clamping base. While that might mean the base is over the damaged edge, it is bigger in the other directions also, which means more/stronger clamping.
I'm not very good at parting.
Mostly because my parting tool is tiny and flexible (MGMN200 inserts in a MGEHR1212-2 holder), but also because I am usually trying to part steel on a lathe that isn't quite rigid enough. (narrow compound slide, narrow cross slide, light weight carriage)
My suggestions;
A) Grab a large flat 2nd cut file, or smooth file, and gently file across the top of the compound slide, to make sure there are no high spots.
B) Always make everything as rigid as possible. Check your saddle gib isn't loose (the strap across the back of the carriage that clamps onto the back of the bed). If the compound is wound toward the chuck, wind it back, so the toolpost is close to the middle of the cross slide. Lock the saddle. If possible, tighten the gib screws, or use a clamp to stop the compound from rattling in its feed screw and dovetail.
C) If your parting tool is juddering/grabbing/twisting;
C1) Make sure your parting tool has clearance. Use a micrometer to make sure the nose width isn't smaller than the slot being cut further back along the tool. Here is a nice diagram from Parting Off on Mini Lathes and Bearing Choices
Parting_Tool.jpg
C2) Make sure your parting tool is perpendicular to the spindle centre.
C3) Try making clearance as you cut. Go in by 2mm, pull back, go left a little, go in by 4 mm, pull back, go right a little, go in my 6mm, et c.
D) For gummy materials (Copper, most Aluminiums), try coolant, oil, talcum powder
You can maybe get another compound top slide casting from Mal:
https://australianmetalworkinghobbyi...ound+top+slide
but unless it is cracked, I wouldn't bother!
-
8th Nov 2021, 10:01 AM #3Diamond Member
- Join Date
- Mar 2011
- Location
- Dural NSW
- Age
- 82
- Posts
- 1,203
Parting off On Hercus lathe
Some years back I installed an extended cross slide to my Hercus 260 lathe & use an inverted rear toolpost for parting off.
This is a very solid & convenient unit as it stays in position clamped all the time, & does not get in the way of conventional turning using the front conventional toolpost.
So all good !
Bruce
-
8th Nov 2021, 08:21 PM #4New Member
- Join Date
- Aug 2021
- Location
- The Rock, NSW, Australia
- Age
- 70
- Posts
- 6
I did some parting off on 9"AR today with a similar tool, but in brazed carbide in a shop made tool holder. Low speed and feed and it went very well. These little lathes are quite something.
Similar Threads
-
Hercus 9" Backing plate for 5" 4 jaw chuck.
By lamestllama in forum WANTED TO BUYReplies: 1Last Post: 14th Sep 2020, 02:45 PM -
Ex Hercus "Asia Planer"
By rickw72 in forum THE HERCUS AREAReplies: 2Last Post: 22nd Apr 2014, 06:34 PM -
WEST AUST Hercus metal lathe 12" x 42" excellent condition
By craig manley in forum METALWORK - Machinery, Equipment, MARKETReplies: 0Last Post: 6th Jul 2011, 02:29 AM -
Bantam Topslide Travel