    Still looking for things to do....

    Recently doing repairs on a few antique fly reels I found that screws are very hard to find. I decided to make some of those screws. Cutting the threads was straight forward; I used the appropriate die. But to cut neat straight slits was a bit more of a challenge as I wanted to use a slitting saw to make positive neat slits. Only problem was that I didn't have the saw or arbor and I even needed a collet block.

    First things first. I decided to make an arbor. Here's how I did it.

    I turned down some 4140 steel to 5/8" for the shaft to fit a 5/8 5C collet as I wanted to hold it in a collet in the spindle.

    Capture 4140.PNG

    After that I turned it around holding it in the 5/8 collet to continue on the other end. This ensured I could keep it reasonably concentric as I proceeded

    20200521_213859.jpg

    20200524_153252.jpg

    After drilling and turning down the cap piece to .0005 smaller to allow the saw blade ID to slide on, I parted off the cap piece and bored out the body to accept the cap internal arbor. Then tapping the body with an M8 thread. I also counter bored the cap for the cap screw.

    20200524_194015.jpg


    20200525_175942.jpg

    Little bit of a taper on the back of the body to reduce weight and make it appear pleasing; a polish up made a good result.

    20200529_140813.jpg

    Now, to cut some screw heads which were held in a 5C collet in a collet holder in the milling attachment on the Hercus

    20200529_143539.jpg


    20200529_145219.jpg

    The slits are a little deep here but now I dial in the right depth.

    The screws were for a reel that is a good 80 years old - JW Young of England.

    20200518_180744.jpg

  2. #2
    Join Date
    Jun 2013
    Location
    Tasmania
    Posts
    257

    Default

    Nice. I use my 9a for slotting screws all the time with the same set up.

    Give us some more info on your fly reel resto's though!

    I've got a JW Young Beaudex on a Hardy cane Palakona 9'. Unfortunately with a broken tip, but would love to find a replacement tip one day.

  3. #3
    Join Date
    Mar 2017
    Location
    Sydney between denial & paranoia
    Posts
    88

    Default

    Quote Originally Posted by Hornetb View Post
    Nice. I use my 9a for slotting screws all the time with the same set up.

    Give us some more info on your fly reel resto's though!

    I've got a JW Young Beaudex on a Hardy cane Palakona 9'. Unfortunately with a broken tip, but would love to find a replacement tip one day.

    I have a few Youngs. I really like them especially the red agate reels although they are all nice examples and workhorse reels.

    Two reels I bought that had damaged check and the other a broken check knob.

    Attachment 393517
    So I set out to repair them. First was the brass rivet pin to allow the spring & pawl to hold in place.

    20181026_210738.jpg

    Here you can see the hole where the rivet should be so it can hold the pawl on place like the other side.


    20181026_210716.jpg

    Below shows the rivet in place with a new Hardy's pawl as I couldn't get hold of an old Young pawl. It's a little bigger but it still fits.

    20181026_215138.jpg


    On the other reel the check tensioner knob was broken so I removed the entire thing including the rivet that holds it in place and made a new head with threaded rod, rivet and stop, so the pressure arm can be screwed up and down to add, or reduce, tension on the spring for more drag.

    20200422_123838_001.jpg

    20200515_134702.jpg

    Below is the old broken assembly and the new remade version

    20200515_145304.jpg

    Here it is prior to putting in the stop

    IMG-3edebe0c3e60350d37874613d74457a2-V.jpg

    Finally the completed repair

    20200518_180725.jpg


    At another time I replaced a cracked agate in another smaller Young reel

    20190505_173902.jpg

    Made a collet stop for the nickel silver bezel. The bezel was then opened with a spinning type of tool then placed a new agate in and closed up the bezel leading edge by rolling it down with the same tool.

    20190511_142956.jpg

    Here you can see another bezel that I repaired to accept a smokey agate for a Hardy St George.

    20181110_132624.jpg

    This is what I used to open the bezel then close it over the agate.

    20181110_132646.jpg

    A rivet made to hold the bezel tang in place on the reel.

    20190511_163747.jpg

    Finally the finished reel.

    20190511_173423.jpg

    here is the Hardy St George repaired also
    20181110_165901.jpg

    This is stop that goes into the collet, you can see the bezel tang also.

    20181110_140153.jpg
    Attached Images Attached Images

  4. #4
    Join Date
    Mar 2017
    Location
    Sydney between denial & paranoia
    Posts
    88

    Default

    Hornet,

    You could get the old tip repaired or have a new one made.

  5. #5
    Join Date
    Jun 2013
    Location
    Tasmania
    Posts
    257

    Default

    Quote Originally Posted by Boris Ludwig View Post
    Hornet,

    You could get the old tip repaired or have a new one made.
    Beautiful work there. I love your stuff.

    Yeah I thought I could get it repaired but haven't had it professionally assessed. I had a gent locally that fixes cane rods look at it and he said it couldn't be done, or wasn't particularly keen to do it perhaps.

    I've had the rod and reel for probably 30 years now. Be happy just to fix it and put it on the wall.

  6. #6
    Join Date
    Mar 2017
    Location
    Sydney between denial & paranoia
    Posts
    88

    Default

    Quote Originally Posted by Hornetb View Post
    Beautiful work there. I love your stuff.

    Yeah I thought I could get it repaired but haven't had it professionally assessed. I had a gent locally that fixes cane rods look at it and he said it couldn't be done, or wasn't particularly keen to do it perhaps.

    I've had the rod and reel for probably 30 years now. Be happy just to fix it and put it on the wall.

    Thanks, Hornet.

    Where are you in Australia or elsewhere? It'd be a nice wall feature, especially in the "pool room" as they say

    Fixing older rods is a specific skill set; very different to making from scratch.

  7. #7
    Join Date
    Oct 2001
    Location
    ACT
    Posts
    667

    Default

    is that actually a 7/64 BSW die? thats an unusual size

  8. #8
    Join Date
    Mar 2017
    Location
    Sydney between denial & paranoia
    Posts
    88

    Default

    Quote Originally Posted by Zsteve View Post
    is that actually a 7/64 BSW die? thats an unusual size

    Yep, exactly right. hard to find those screws.

    I was lucky to find the die & tap in 7/64 BSW, unused I might add.

  9. #9
    Join Date
    Sep 2012
    Location
    York, North Yorkshire UK
    Posts
    6,480

    Default

    Hi Guys,

    7/64 Whit, almost as rare as rocking horse poo !

    I would imagine 2.5 mm or 3 mm would have been used today !

    Nice work on your reels by the way, works of art
    Best Regards:
    Baron J.

  10. #10
    Join Date
    Mar 2017
    Location
    Sydney between denial & paranoia
    Posts
    88

    Default

    Quote Originally Posted by BaronJ View Post


    Nice work on your reels by the way, works of art

    Thanks, BaronJ.

    The real "works of art" will be realised when I make one from scratch.

  11. #11
    Join Date
    Mar 2017
    Location
    Sydney between denial & paranoia
    Posts
    88

    Default

    Quote Originally Posted by Hornetb View Post
    Nice. I use my 9a for slotting screws all the time with the same set up.

    Give us some more info on your fly reel resto's though!

    I've got a JW Young Beaudex on a Hardy cane Palakona 9'. Unfortunately with a broken tip, but would love to find a replacement tip one day.

    Hornet, got any photos of your screw slot cutting on the 9?


    I have a nice Beaudex and a Pridex too. Beaudex is a great reel. Pridex on the right second going left is the Beaudex.


    20181028_093613.jpg

    Beaudex in the foreground

    P1040636.jpg

Similar Threads

  1. 22 mm Slitting Saw Arbor
    By electrosteam in forum WANTED TO BUY
    Replies: 5
    Last Post: 10th Aug 2020, 09:32 PM
  2. multi bore slitting saw arbor problem
    By tanii51 in forum TIPS, TRICKS & HOW TO'S
    Replies: 6
    Last Post: 13th Dec 2013, 09:11 AM
  3. CTC arbor for slitting saw
    By eskimo in forum METALWORK GENERAL
    Replies: 1
    Last Post: 18th Feb 2013, 10:58 AM
  4. Slitting saw arbor
    By morrisman in forum METALWORK GENERAL
    Replies: 10
    Last Post: 21st Sep 2011, 09:30 PM
  5. ISO30 or NMTB30 Slitting Saw Arbor- I'm looking for one.
    By Anorak Bob in forum METALWORK GENERAL
    Replies: 8
    Last Post: 9th Sep 2011, 02:15 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •