    I have dug up what previous threads I can on running temperatures of the bearings in the vertical head of Model 0 mill. It seems that they do run rather hot.
    My question is while the temps noted in the threads may not be ideal, what are the limits? Given the Hercus Mills were designed the way they are, it would seem they have been operating at the temps they do since manufacture. At what point of temp should one worry?

    My test run time of 5 mins @ 1400 rpm fro 35 to 41 C 10 minutes upto 43 c

    TH

  2. #2
    Join Date
    Sep 2012
    Location
    York, North Yorkshire UK
    Posts
    6,481

    Default

    Hi TH,

    Whilst my mill is not a Hercus, it does use a pair of tapered bearings at each end of the spindle, they get warm but not hot ! It might pay you to strip clean and re-lubricate them. When I sorted mine out I used a lithium based wheel bearing grease, the old stuff was like a thick toffee making the spindle hard to turn by hand. Washing them out in white spirits cleaned them nicely.

    Don't repack the bearings full ! Only about 50% is needed.

    HTH.
    Best Regards:
    Baron J.

  3. #3
    Join Date
    Oct 2019
    Location
    Nth Queensland
    Posts
    55

    Default

    Thanx all have fesolved my query pls disregard post
    Last edited by Tham60; 22nd Apr 2021 at 01:52 PM. Reason: resolved

Similar Threads

  1. Replies: 0
    Last Post: 3rd Jul 2020, 04:15 PM
  2. Rambaudi V2 vertical milling head
    By Slatept in forum METALWORK GENERAL
    Replies: 4
    Last Post: 21st Oct 2019, 10:17 PM
  3. Hercus Vertical Head.
    By stix012 in forum THE HERCUS AREA
    Replies: 4
    Last Post: 12th May 2015, 08:05 AM
  4. Hercus Model O Vertical Head Clearance
    By gdonald in forum THE HERCUS AREA
    Replies: 14
    Last Post: 16th Jun 2014, 08:45 AM
  5. What's in a vertical head?
    By neksmerj in forum METALWORK GENERAL
    Replies: 25
    Last Post: 19th Apr 2011, 05:11 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •