If the thread you cut was not 1.5 but what was set on the gearbox you may not of been able to drop in anywhere.
Sent from my T85 using Tapatalk
-
26th Dec 2020, 06:07 PM #17
Success!
But I can't figure out what caused the problems before except your suggestion, Pipeclay.
But that means I had something askew in my settings because this time I still just dropped in without reference to the thread dial and I did open the halfnuts at the shoulder.
20201226_172611.jpg
20201226_175520.jpg
Thanks to those who posted suggestions and all the best for the New Year.
-
31st Dec 2020, 12:13 PM #18
Task complete, finally finished the caps to go with them.
20201231_113829.jpg
Actually, it was learning exercise cutting an internal thread into a blind hole and finishing the outside.
-
31st Dec 2020, 09:26 PM #19
Hi Boris, Guys,
If the thread being cut is a multiple of the leadscrew then you can drop in anywhere ! This applies to an imperial machine and I assume metric as well.
Cutting threads in a blind hole, its safer to cut from the inside out away from the chuck.
Anyway from the pictures it looks to be all good.Best Regards:
Baron J.
-
1st Jan 2021, 04:08 PM #20Most Valued Member
- Join Date
- Nov 2007
- Location
- melbourne australia
- Posts
- 3,228
Nice job.
Chris
-
2nd Jan 2021, 08:25 AM #21australian metalworking hobbyist
- Join Date
- Jan 2009
- Location
- Holbrook, NSW
- Age
- 73
- Posts
- 490
5H592.jpg
quite correct, the line was repositioned later, as shown on the current new plates.
Similar Threads
-
Imperial and Metric Bolt Thread and Torque Chart
By moorebrm in forum METALWORK GENERALReplies: 5Last Post: 31st May 2016, 01:48 AM -
Printable imperial-metric-bolt-thread-torque-chart
By moorebrm in forum CONVERSIONS & CALCULATIONSReplies: 0Last Post: 16th May 2016, 09:03 PM -
Gas Thread info needed
By ericg in forum METALWORK GENERALReplies: 5Last Post: 12th Jan 2015, 01:31 PM -
ACME thread chart
By morrisman in forum METALWORK GENERALReplies: 1Last Post: 7th Aug 2012, 09:48 PM -
AL-340A Thread Chart Misprint
By matthew_g in forum METALWORK GENERALReplies: 1Last Post: 12th Jul 2010, 08:32 AM