Chuck Indexer
I drilled 12 holes in the backplate of my 3 jaw chuck using my indexing attachment and cross-slide mounted drill. I made a pin from 10mm W1 with a slightly tapered tip. The brass knob has a M12 thread which forces the pin into the 4mm holes in the chuck. I remove the pin when I want to fit the 4 jaw chuck. I need to remove the whole assembly (two cap screws) on the rare occasion I use the face plate.
My original indexer will still be needed for the 4 jaw chuck, collet chuck and face plate. The advantage of this indexer is that it requires no setup when you just want to make 2, 3, 4 or 6 holes/slots in a workpiece.Chris
Similar Threads
-
spin indexer
By shedhappens in forum METALWORK PROJECTSReplies: 13Last Post: 6th Mar 2020, 10:37 PM -
What is this ? Lathe bed indexer or something else ?
By MasterSpoon in forum METALWORK GENERALReplies: 3Last Post: 6th Dec 2017, 08:25 PM -
Newbould Indexer
By Machtool in forum METALWORK GENERALReplies: 15Last Post: 13th Jul 2017, 03:36 PM -
Solar panel indexer
By Steamwhisperer in forum METALWORK PROJECTSReplies: 32Last Post: 8th May 2016, 08:23 PM -
Hercus Indexer - Photos for Joe.
By Anorak Bob in forum METALWORK GENERALReplies: 13Last Post: 4th Mar 2012, 12:18 PM