Page 2 of 2 FirstFirst 12
Results 16 to 26 of 26
  1. #16
    Join Date
    Jan 2009
    Location
    Holbrook, NSW
    Age
    73
    Posts
    490

    Default big bore

    Quote Originally Posted by Tinkerer77 View Post
    I have a couple of photos of the lathe now, I do wonder how many others were ordered with the D1-4 option at $890.00 + GST. that is 2 known of now, there could be more out there in workshops.
    Hi Steve,
    There won't be any with the big bores you two have, just the standard would have been offered in the Axmell list. Unless another shows up, yours are unique, with the exception of the 50 gs-26 in the USA.
    Mal

  2. #17
    Join Date
    Jan 2009
    Location
    Holbrook, NSW
    Age
    73
    Posts
    490

    Default who wants a D1-4 spindle for their 260

    Quote Originally Posted by Boris Ludwig View Post
    Here's a copy of a page from the 2000 price list where you can see the Camlock D1-4 spindle listed as an optional extra.

    Attachment 386603

    I have an earlier price list from 1988 that does not list the camlock
    I am trying to find out if there is any appetite amoung 260 owners for the D1-4 spindle. This isn't the large bore variety, that Boris and Steve have on their GS-26 models, just the standard bore. It is possible that Hercus may be willing to make a batch, if the numbers are there. This should be a straight replacement for the standard threaded spindle. It would be nice, to be able to run the lathe in either direction without having to risk it unscrewing. The price, as you can see by the pricelist, will be a shocker.
    For 9" owners, it will have to wait until we see how this goes.

  3. #18
    Join Date
    Nov 2007
    Location
    melbourne australia
    Posts
    3,228

    Default

    Quote Originally Posted by allterrain50 View Post
    It would be nice, to be able to run the lathe in either direction without having to risk it unscrewing.
    It sure would.

    Quote Originally Posted by allterrain50 View Post
    The price, as you can see by the pricelist, will be a shocker.
    I reckon it would be worth whatever it costs just for the safety improvement. But I'm worried about how much work is involved in the changeover. And I'd need to make new backing plates for my chucks. Might as well get new chucks if I'm going to the trouble. And my ER40 collet chuck would become a paperweight. I could sell that I guess.

    Put me down as a "maybe" Mal.
    Chris

  4. #19
    Join Date
    Mar 2017
    Location
    Sydney between denial & paranoia
    Posts
    88

    Default

    Jack, just after I bought my lathe I was slightly disappointed when I realised that parts and attachments were not going to be readily available and I'd need to be patient.

    But soon after I found various leads to southbend parts and info that helped me slowly and incrementally gather information and tooling. That helped me realise what a great machine I now have. Sure I have the big bore which allows 5C collects to be used realitively cheaply without resorting to inaccurate Chinese 5C chucks.

    In the case of the regular size bore 3C collects would be the norm.

    Perhaps your ER would still be able to be used if properly modified with a draw bolt. A drawbolt would be relatively easy to make.

    I now think I was fortunate to have been in the right place to find this lathe. At work I sometimes use a threaded spindle Hercus 260 which was my first intro to Hercus and metal lathes. I can tell you that I prefer the D 1-4.

    So this opinion may not be shared by most for lots of considerations. Also take it for what it is, just an opinion of a self-taught relative novice.

  5. #20
    Join Date
    Nov 2007
    Location
    melbourne australia
    Posts
    3,228

    Default

    Quote Originally Posted by Boris Ludwig View Post
    Perhaps your ER would still be able to be used if properly modified with a draw bolt. A drawbolt would be relatively easy to make.
    Hi Boris,
    My collet chuck screws onto the Hercus 260 spindle nose and allows stock of any length to be gripped. It's fantastic. A draw-bar is not an option with this chuck. I also have my original ER40 collet chuck with a MT4 shank which I use with a draw-bar. It can safely be used in reverse, but can only hold short stock.
    Chris

  6. #21
    Join Date
    Aug 2015
    Location
    Adelaide
    Posts
    240

    Default

    Hi Boris

    The 5c collets were an option on the standard 260, I have a 5c draw tube that came with my long bed, the closer was missing from my head stock and I have not been able to track one down as yet but I will keep looking.

    Mal

    I would be keen on changing over my standard 260 to a D1-4 spindle on my long bed, definitely a nicer system than the screwed nose and less back gear breaking issues trying to undo stuck chucks.

  7. #22
    Join Date
    Nov 2007
    Location
    melbourne australia
    Posts
    3,228

    Default

    Quote Originally Posted by Tinkerer77 View Post
    …less back gear breaking issues trying to undo stuck chucks.
    Good point.
    Chris

  8. #23
    Join Date
    Nov 2007
    Location
    melbourne australia
    Posts
    3,228

    Default

    And I guess I’d need a new faceplate and dog plate. I think the total cost of the changeover could be quite expensive.
    Chris

  9. #24
    Join Date
    Mar 2017
    Location
    Sydney between denial & paranoia
    Posts
    88

    Default

    Quote Originally Posted by Tinkerer77 View Post
    Hi Boris

    The 5c collets were an option on the standard 260, I have a 5c draw tube that came with my long bed, the closer was missing from my head stock and I have not been able to track one down as yet but I will keep looking.
    Ok, I wasn't aware of that the 4 Hercuses here at college all have 3C collet attachments and they all have a standard spindle with thread. Thanks for the info.

  10. #25
    Join Date
    Mar 2017
    Location
    Sydney between denial & paranoia
    Posts
    88

    Default

    Quote Originally Posted by jack620 View Post
    Hi Boris,
    My collet chuck screws onto the Hercus 260 spindle nose and allows stock of any length to be gripped. It's fantastic. A draw-bar is not an option with this chuck. I also have my original ER40 collet chuck with a MT4 shank which I use with a draw-bar. It can safely be used in reverse, but can only hold short stock.
    Ok, I see what you mean if it screws directly onto the spindle threads.

    I guess there are specifics for each situation. Thanks again for the info.

  11. #26
    Join Date
    Jan 2009
    Location
    Holbrook, NSW
    Age
    73
    Posts
    490

    Default D1-4 spindles

    Quote Originally Posted by allterrain50 View Post
    I am trying to find out if there is any appetite amoung 260 owners for the D1-4 spindle. This isn't the large bore variety, that Boris and Steve have on their GS-26 models, just the standard bore. It is possible that Hercus may be willing to make a batch, if the numbers are there. This should be a straight replacement for the standard threaded spindle. It would be nice, to be able to run the lathe in either direction without having to risk it unscrewing. The price, as you can see by the pricelist, will be a shocker.
    For 9" owners, it will have to wait until we see how this goes.
    Bad news, Having talked to Hercus There is no possibility of remaking the D1-4 spindle anywhere near the 2000 price and I am therefor abandoning the project as impractical.
    Mal

Page 2 of 2 FirstFirst 12

Similar Threads

  1. Show us your Shaper
    By Bryan in forum METALWORK GENERAL
    Replies: 528
    Last Post: 25th Apr 2018, 10:11 PM
  2. Hercus Mill Spindles
    By SurfinNev in forum THE HERCUS AREA
    Replies: 19
    Last Post: 21st Sep 2011, 09:56 PM
  3. Materials used on Threaded lathe spindles.
    By pipeclay in forum METALWORK GENERAL
    Replies: 7
    Last Post: 4th Jul 2011, 07:51 PM
  4. Chasing Old Crosslide spindles
    By bitza500 in forum THE HERCUS AREA
    Replies: 2
    Last Post: 20th Nov 2008, 07:25 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •