Cylindrical grinding a tap on my Hercus
Toolmaker needs to tap 30mm M6 into Aluminium, and is as cheap as me. Instead of one of us doing a hack job on a bench grinder (one of these days I'll make a jig), decided to setup my Hercus with a little grinder.
Started with the chuck:
IMG_0647.jpg IMG_0648.jpg
but the runout was terrible, so made use of one of Peter's collet holders:
IMG_0653.jpgIMG_0649.jpg
Failed to get a good action shot showing any sparks, but I was going VERY slowly – only 2 or 3 thou off each pass, and mostly hand feeding because my slowest auto feed was too much. End result pretty good:
IMG_0660.jpg
About 1mm off the wheel diameter, and about the same off the tap shaft!
There is a slight step, more runout further away from the collet.
Might be a bent tap, might be my imperfect collet taper machining.
Similar Threads
-
Hercus 9 cylindrical grinder
By smxas in forum METALWORK GENERALReplies: 7Last Post: 28th Oct 2014, 11:51 AM -
cylindrical grinding on a TCG
By bob ward in forum METALWORK GENERALReplies: 13Last Post: 3rd Sep 2014, 11:24 AM -
Hercus 9A Cylindrical Grinder
By Anorak Bob in forum THE HERCUS AREAReplies: 5Last Post: 21st Apr 2012, 10:48 PM -
DONE: Hercus Cylindrical grinder
By azzrock in forum METALWORK - Machinery, Equipment, MARKETReplies: 6Last Post: 15th Feb 2012, 03:12 PM -
Hercus 9a Cylindrical Grinder
By xXvapourXx in forum METALWORK GENERALReplies: 5Last Post: 2nd Nov 2011, 10:03 PM