Cutting a 2mm pitch 3/8 acme thread
So I'm up to cutting the thread on the replacement compound feed screw.
Putting the gearbox in 2mm pitch mode works for a normal triangular thread, but looks way too small for the acme thread.
Should I be using a different pitch or feed rate for acme thread? The gearbox mentions 50 or 20 stud gear. Which one is that?
I haven't done a lot of threading to date. I'm also going to put a forward and reverse switch on the lathe as I don't have a threading dial.
Any pro tips?
Martin
Sent from my H4133 using Tapatalk
-
2nd Sep 2019, 07:27 PM #2Most Valued Member
- Join Date
- Jun 2007
- Location
- sydney ( st marys )
- Age
- 64
- Posts
- 4,890
Take the 20 off the stud and take the 50 off the screw, put the 50 on the stud and the 20 on the screw, engage the 50 with the 80 and the 45, use the 20 as the spacer on the screw.
-
2nd Sep 2019, 07:32 PM #3Intermediate Member
- Join Date
- May 2016
- Location
- AU
- Posts
- 30
Awesome, easy to understand instructions that directly answer my question.
Thanks Pipeclay.
Sent from my H4133 using Tapatalk
-
3rd Sep 2019, 09:59 PM #4Member
- Join Date
- Nov 2015
- Location
- Brisbane Australia
- Posts
- 85
This You Tube clip might be helpful
https://www.youtube.com/watch?v=df-7...ature=youtu.be
-
6th Sep 2019, 06:24 PM #5Intermediate Member
- Join Date
- May 2016
- Location
- AU
- Posts
- 30
So thanks to the help of pipeclay I set up the change gears, ground a hss tool, and had a go at cutting the acme thread.
I was happy with this for my first go. I'll cut another one for practice before I have at my blank.
Before I do, though, I really need to get a fwd/reverse switch. Rolling the chuck backwards after each pass got old pretty quickly. Anyone in Melbourne got a source for this kind of switch gear? I'm running a 1hp single phase motor through a DOL switch. Any issues I should consider?
Martin
Sent from my H4133 using Tapatalk
-
10th Sep 2019, 10:31 PM #6Most Valued Member
- Join Date
- Oct 2010
- Location
- melbourne, laverton
- Posts
- 1,910
star wheel
if your in melbourne you can borrow my star wheel if you like.
aaron
-
11th Sep 2019, 03:52 AM #7
Hi Guys,
If a star wheel is what I think it is, I made one using an old washing machine drum pulley.
21022015-01.JPG 21022015-05.JPG
You tighten the nut to expand the collet inside the lathe spindle.
Another turning job.Best Regards:
Baron J.
-
11th Sep 2019, 10:13 AM #8Most Valued Member
- Join Date
- Jun 2007
- Location
- sydney ( st marys )
- Age
- 64
- Posts
- 4,890
I maybe wrong but I think the Star wheel mentioned is referring to the Thread Chasing Dial.
-
11th Sep 2019, 10:31 AM #9Senior Member
- Join Date
- Oct 2010
- Location
- NSW
- Posts
- 181
No wheel at all on my version. I made the expanding collet and use my cordless drill to reverse back to the start of the thread.
-
11th Sep 2019, 10:34 AM #10Intermediate Member
- Join Date
- May 2016
- Location
- AU
- Posts
- 30
I thought it was a reference to the giant ferris wheel down at Docklands.
I'll probably make something like that expanding arbor. I think I actually have something like that from an old washing machine myself! I like to use these bits and pieces so that I can prove that keeping it was worthwhile, despite what others in my household might say...
Unless I find a fwd/reverse switch first. Or buy a thread dial from Mal.
Martin
Sent from my H4133 using Tapatalk
-
11th Sep 2019, 06:42 PM #11
-
15th Sep 2019, 11:28 PM #12Most Valued Member
- Join Date
- Oct 2010
- Location
- melbourne, laverton
- Posts
- 1,910
threading dial
as usual pipe clay was on the money.
i was talking about a threading dial.
aaron
-
29th Sep 2019, 01:44 PM #13Senior Member
- Join Date
- Aug 2012
- Location
- Greenmount, W.A.
- Age
- 70
- Posts
- 275
It is Sunday, so brain not engaged yet, but.........
Hercus Compound screw is a Left Handed thread. The photo showing the two threads are different hands or are they?
-
29th Sep 2019, 01:51 PM #14Most Valued Member
- Join Date
- Jun 2007
- Location
- sydney ( st marys )
- Age
- 64
- Posts
- 4,890
Yes the Cross Slide screw and Compound screw are different, they are Left and Right handed.
-
1st Oct 2019, 08:07 PM #15
Acme or Trapezoidal
I am curious Acme threads are imperial only.
The metric version is trapezoid.
Not much different to look at but the metric screw has 15 degree flanks and a included angle of 30° not 29° like a Acme thread.
Are they really Acme threads with a 2mm pitch?
MarkI've become a tool of my tools.
Similar Threads
-
ACME thread in Oz
By kenny_10 in forum METALWORK GENERALReplies: 9Last Post: 28th Jun 2019, 07:29 PM -
ACME thread
By SAISAY in forum CNC ForumReplies: 2Last Post: 17th Aug 2016, 12:08 PM -
Hercus front oiler thread pitch and dimensions?
By neevo in forum THE HERCUS AREAReplies: 25Last Post: 21st Apr 2014, 01:42 PM -
ACME thread gauge
By Grahame Collins in forum METALWORK GENERALReplies: 8Last Post: 21st Oct 2012, 08:27 AM -
ACME thread chart
By morrisman in forum METALWORK GENERALReplies: 1Last Post: 7th Aug 2012, 09:48 PM