Needs Pictures: 0
Results 1 to 15 of 18
Thread: Hercus 270 Shaper
-
19th Sep 2016, 03:22 PM #1
Hercus 270 Shaper
Some photos of my new Hercus 270 Shaper.The machine is ex school and in great condition.Not sure of it's actual age but it may be mid to late 80's.
The Shaper is metric in all its feed screws and dials.
So far it has just had a good clean and re-oil and adjust the sliding ways.I have been grinding a few tools to what I think will work and then fine tuning from there.Classic case today was a shear cut tool which wasn't very good.I increased the clearance angle from 10 to 15 degrees and it now works fine.This is the tool that produced the curly chips and surface finish in the last of these photos.
The machine runs very quietly and performs well, like all Hercus machines.Micheal.
-
19th Sep 2016, 05:07 PM #2Intermediate Member
- Join Date
- Apr 2016
- Location
- New South Wales
- Posts
- 45
What a ripper !
-
19th Sep 2016, 06:43 PM #3
Just uploaded a little video look at the new shaper having a test run.
Micheal.
-
19th Sep 2016, 07:16 PM #4Novice
- Join Date
- Jan 2014
- Location
- Perth, Western Australia
- Posts
- 18
Very nice Localele. I too have a 270 but not being in as good shape as yours, is currently being overhauled. Mine has serial number 4Q-2929. Here's a picture of progress to date.
H270_Sept.JPG
-
19th Sep 2016, 07:29 PM #5
I forgot the serial number which is 4Q-2885. I have no idea how many of these were made.May prove interesting if someone knows both their serial number and a date of purchase.This may help us to date some other machines a bit closer.
Micheal.
-
19th Sep 2016, 08:07 PM #6Novice
- Join Date
- Jan 2014
- Location
- Perth, Western Australia
- Posts
- 18
Thanks Michael, yes that would be of interest to me too. This link has a few additional details.
//metalworkforums.com/f189/t178...haper-manuals?
Rod.
-
4th Oct 2016, 02:50 PM #7Novice
- Join Date
- Jan 2014
- Location
- Perth, Western Australia
- Posts
- 18
Hello folks.
As the Hercus 270 shaper has come up on this forum, I'm hoping that you good people may be able to help me out?
I don't understand how the vertical slide lock is supposed to work. Perhaps someone can give me an insight?
The casting with the red cavity is the cross rail (or bridge) which slides vertically on a 60 degree vertical dovetail on the front of the main casting.
front.jpg
It is jacked up and down by the jacking screw that can be seen. This movement does not (normally!) occur under cut. The table height is adjusted and then locked off for the duration of the actual cut. So the lock must function firmly. All of the cutting reaction forces (horizontal and vertical) pass through this locked up dovetail. In the view in the photo, the left side is a fixed dovetail and the right side has an adjustable gib. (I know that the cross rail is also supported on the jacking screw, but don't believe that should be relied upon.)
The design of the gibbed side, when looking down from above, is like this.
sketch.jpg
The bolt holes through the gib have plenty of clearance. Both the upper and lower ends of the gib have a pair of locking bolt and associated adjusting screw. In the centre of the gib's span is a hole that fits over a through stud (the stud is fixed into the cross rail and protruds backwards) onto which the locking nut and handle screws.
side_of_gib.jpg
Here's the stud when viewed from above...
stud.JPG
The gib's contact surfaces look like this...
gib.JPG
Important note: The three machined pads were all machined at one setting and are all in the same plane.
I can adjust the gib nicely for a good sliding fit on the dovetail. The last part of that adjustment is to tighten the two bolts and so the upper and lower machined pads are pulled tight onto the mating surface of the cross rail and that also enforces the correct orientation of the gib so that the angled surfaces then align correctly.
So now to the question.
When adjusted in that way, the centre pad, under the locking nut handle, is already in contact with the mating surface (all pads are in same plane) and won't move any appreciable amount when the locking nut is tightened. Hence no locking action can occur? (I get a very slight increase in friction, but that is probably just the oil film being squeezed a little thinner.)
What have I missed? Any ideas on how the lock is supposed to work would be appreciated!
I notice that the lock on the Douglas machines (the 270 was derived from the Douglas) has the locking nut in the upper position. (for example, see this Youtube at about 0:09 seconds onwards. https://www.youtube.com/watch?v=VC8KR9ing0w ) Perhaps someone with a Douglas can take some photos of the gib arrangement on that machine for me? Is the gib solid or split with a saw cut in some way? Is the lock on the Douglas effective? If so, how does it differ from the 270 design?
Many thanks in advance.
Rod.
-
4th Oct 2016, 04:30 PM #8
Hi Rod, The lock in use is fine from what I can see.While it doesn't completely weld the table slide it still does it's job of tightening the jibs.Remember for the table to slide down it must overcome a few hurdles.First is the locking handle.Second it has to be able to rotate the pinion drive on the height adjuster to allow any movement and third it would also have to bypass the front table support arm pictured below.
I did just try mine and while the crank handle can overcome the lock to lift the table it is would not be an issue for normal use.Obviously pretty hard to crank it down past the front support.
IMG_3827.jpg IMG_3830.jpgMicheal.
-
5th Oct 2016, 12:34 AM #9Novice
- Join Date
- Jan 2014
- Location
- Perth, Western Australia
- Posts
- 18
Thanks for doing those tests Michael. It confirms that your lock is also not very firm. And I don't really see how they can be with this design.
It will be interesting to see what the Douglas owners say.
Thanks again.
Rod.
-
5th Oct 2016, 07:02 AM #10
The table would be solid.The lock is only there to help stop the table from sagging when it is extended out fully right or left by tightening the jib strip.
Once you get it back together you could check with an indicator if the table sags when fully extended.Check with and without the lock done up.Micheal.
-
12th Oct 2016, 04:55 PM #11.
- Join Date
- Nov 2008
- Location
- Perth WA
- Age
- 71
- Posts
- 6,459
Micheal and Rod,
The gib lock on my Douglas is pretty much ineffective. I had a fiddle with the gib adjustment screws and detected no difference lock-wise with them tight or loose. On the other hand, the gib lock I fitted to my very early No.0 mill works very effectively. Hercus did not provide a lock on the mill in the early days. The gib design is similar to that used by Douglas albeit the obvious one screw less.
BT
DSC_6836 (Large).JPG DSC_6833 (Large).JPG DSC_6845 (Large).JPG
-
13th Oct 2016, 12:36 PM #12Novice
- Join Date
- Jan 2014
- Location
- Perth, Western Australia
- Posts
- 18
Hi Bob,
Many thanks for taking the time to do the tests and to take the photos. Very interesting result.
May I ask a few additional questions?
On your Douglas, near the top of the gib, I can see a square-headed set screw. Does this prevent rotation of the hex-headed bolt that is at right angles to it? And is the locking handle screwed onto that same bolt?
In addition, I can see 3 pairs of adjusting screws (hex head) and clamping bolts (hex head).
Is the gib's clamping surface (not the dovetail surface) flat, or does it have the 3 pads as per my last photo in 4th Oct post?
The lock on your No. 0 mill. Have you replaced the upper adjusting screw with the locking handle and screw that, upon rotation, pushes the gib onto the dovetail? If so, is the upper gib clamping bolt (visible in the shadows on the left) left only 'nipped' so that the gib is free to move when the locking handle is rotated?
Apologies for all the questions and I appreciate your time.
Regards,
Rod.
-
13th Oct 2016, 05:08 PM #13.
- Join Date
- Nov 2008
- Location
- Perth WA
- Age
- 71
- Posts
- 6,459
Hello Rod,
You have described everything exactly as it is on both the shaper and the mill. I removed the Douglas' gib and lock for a few more photos....
DSC_6848 (Large).JPG DSC_6862 (Large).JPG DSC_6858 (Large).JPG DSC_6859 (Large).JPG DSC_6863 (Large).JPG
Reassembled and with an indicator mounted on the table close to the Z dovetail with its stylus on the dovetail, I adjusted the gib screws. Loose enough to raise and lower the table easily and there is about 0.002" play. Obviously there would be considerably more movement in the table if the play was measured from the outer end of the table. With the gib screws tightened to provide about half thou play the table is very hard to move. The last photo suggests a possible solution. Tightening the existing screw in that position locks the table rigidly, the same effect as achieved with the Kipp handle on the mill. When using the mill and raising and lowering the knee while cutting I use to have the lever positioned so there was some drag in the gib. Not enough to impinge on the knee's movement but enough to remove any slop. Worked well enough.
And, forget the apologies.
Bob.
-
13th Oct 2016, 09:33 PM #14Banned
- Join Date
- Aug 2015
- Location
- QLD
- Posts
- 735
A bit of thread drift.
Fred and his Douglas. Fast foward to the 2:40 mark. https://m.youtube.com/watch?v=EEzuaN8c2FU
-
13th Oct 2016, 09:57 PM #15Novice
- Join Date
- Jan 2014
- Location
- Perth, Western Australia
- Posts
- 18
Thanks Bob! Great info and photos that answer my questions. I appreciate the time you have spent exploring for me.
I'll now ponder what, if anything, to do about the "non-locking" lock.
I'll also post a photo when I've finished the reassembly. I'm a bit slow as I'm remanufacturing some parts and doing various mods as I go.
Rod.
Similar Threads
-
Douglas/Hercus shaper vice maybe.
By stix012 in forum EBAY, GUMTREE, and other off forum sales sitesReplies: 0Last Post: 17th Aug 2016, 09:23 PM -
Second shaper job
By TheNutter in forum METALWORK GENERALReplies: 2Last Post: 18th Sep 2015, 09:16 PM -
First shaper job
By TheNutter in forum METALWORK GENERALReplies: 9Last Post: 9th Sep 2015, 11:21 PM -
Hercus/Douglas Shaper manuals?
By TAFE student in forum THE HERCUS AREAReplies: 9Last Post: 25th Jan 2014, 08:29 PM -
TOS shaper
By Bryan in forum METALWORK GENERALReplies: 91Last Post: 16th Mar 2011, 05:58 PM