30th Jun 2014, 04:24 PM #1Diamond Member
- Join Date
- Mar 2011
- Location
- Dural NSW
- Age
- 82
- Posts
- 1,203
Cross Slide Scraping Hercus 260
Had a visit from Mal of Australian Metalworking Hobbyist this morning.
We dismantled the Extended Cross Slide on my Hercus 260 Lathe to examine & get some dimensions.
Anyway while it was apart, checked it for flatness, it had 3 thou (.003") lengthwise convex on its base slide.
Spent the last 3 hours scraping it flat using the granite surface plate & blue.
Then scraped the cross slide saddle to match. This section was surprisingly flat & accurate, requiring little attention
The Extended Cross Slide had obviously moved over time, through stress relief.
All is now good !!!
Learnt a lot in the Scraping Course in Melb. (Thanks Phil) a couple of years back.
regards
Bruce
-
12th Jul 2014, 09:16 AM #2Pink 10EE owner
- Join Date
- Aug 2008
- Location
- near Rockhampton
- Posts
- 6,216
How straight is the dovetail now?
Gold, the colour of choice for the discerning person.
-
17th Jul 2014, 08:44 AM #3
Practice is the best thing for mastering those skills Bruce.My cross slide is available as a tool to further hone your skills anytime.Always remember I am only offering to help you out.There is not much in it for me.
Well maybe a super refined cross slide with deadly accurate action but who's counting.Micheal.
-
14th Nov 2014, 05:06 PM #4Diamond Member
- Join Date
- Mar 2011
- Location
- Dural NSW
- Age
- 82
- Posts
- 1,203
Cross Slide Scraping
RC
Your question of accuracy, has been on my mind, so because its 40 degrees here today & too hot to do any work outside, took a few hours to finish the Hand Scraping job, on the Hercus Extended Cross Slide
The Saddle was accurate, so I scraped the dovetails on the Extended Cross Slide using the Saddle & its cross slide section as a master.
It took a while to scrape the dovetails, however all is now good !!
Better than new.
regards
Bruce
Similar Threads
-
Backlash in Hercus 260 cross-slide
By jack620 in forum THE HERCUS AREAReplies: 15Last Post: 4th Mar 2013, 06:19 PM -
Cross slide scraping
By Stustoys in forum METALWORK GENERALReplies: 358Last Post: 13th Jan 2013, 10:08 PM -
Extended Cross Slide Casting for Hercus
By bwal74 in forum METALWORK GENERALReplies: 33Last Post: 30th Dec 2012, 12:38 PM -
Hercus 260 Cross-slide play
By jack620 in forum THE HERCUS AREAReplies: 19Last Post: 26th Sep 2011, 08:47 PM -
Hercus Extended Cross Slide Casting
By Swarfmaker1 in forum THE HERCUS AREAReplies: 7Last Post: 3rd Dec 2010, 07:18 AM