Maximum workpiece weight for a 260 lathe
G'day all, I've got a bit of 45/90 4140 hollow bar about 400 long to turn into a machine spindle, but i'm a bit worried i may be over taxing my poor old 260. Does anyone know the weight limit for the Hercus 260 work piece? Thanks in advance.
Cheers
-
30th Jul 2013, 10:25 AM #2Most Valued Member
- Join Date
- Jun 2007
- Location
- sydney ( st marys )
- Age
- 64
- Posts
- 4,890
No idea as to the weight the spindle can handle.
I have machined solid at 75mm OD 400 long without a problem on an 9" so what your doing shouldn't be a concern for an 260.
-
30th Jul 2013, 10:40 AM #3New Member
- Join Date
- Nov 2011
- Location
- NSW
- Age
- 46
- Posts
- 8
Thanks Pipeclay, I was hoping it would be ok, i guess i'll just take it nice and slow with lite cuts and hope for the best.
-
30th Jul 2013, 10:53 AM #4.
- Join Date
- Nov 2008
- Location
- Perth WA
- Age
- 71
- Posts
- 6,459
Depends on what you intend turning on the bar. You may be able to use a steady to share some of the load.