3.5T Flat deck trailer build
Made a start tonight.
Was really pleased with my angle cutting and welding - until I realised I’d put the angle at 3600 from the front - instead of 3900 that I intended it to be :(
Thought briefly about splicing the missing 300mm onto the front of it, but have decided just to leave it as is and have the 1200 beaver tail section instead of 900.
https://uploads.tapatalk-cdn.com/202...7a8916a7e2.jpg
What’s the standard practice for the angle join.
Its got a full penetration butt weld on sides and bottom (I didn’t cut the top) and I’m thinking about adding some 3mm plates either side.
Overkill perhaps?
Steve