Forks for Deere Tractor
Hi All,
A while back I needed a light weight but strong carrier and forks for my small JD 1 series tractor. The lift capacity on these machines is not huge, and while quite a bit higher than the equivalent Kubota every kg counts. The lightest forks I could buy at the time was around 140kg including the carrier. I really wanted a set of Artillian forks from the USA but the cost of getting them here was prohibitive.
So, I decided to make something that was pretty close to the Artillians myself. Here's a few photos of the build process and the finished product all painted up in Deere green (grey on the forks). The total weight of the finished forks came in at 54kg which I was very happy with. They have lifted well over 400kg many times without issue.
IMG_5366.JPG IMG_5365.JPG IMG_5364.JPG
-
18th Jun 2020, 11:27 PM #2Most Valued Member
- Join Date
- May 2011
- Location
- Murray Bridge S Aust.
- Age
- 71
- Posts
- 5,959
Nice work, what did you use for the tines/forks?
KrynTo grow old is mandatory, growing up is optional.
-
18th Jun 2020, 11:28 PM #3Most Valued Member
- Join Date
- Nov 2017
- Location
- Geelong, Australia
- Age
- 57
- Posts
- 2,666
Nice work !!
What did you use to make the forks themselves, and did you do anything special at the bend from vertical to horizontal?
Steve
-
19th Jun 2020, 01:55 AM #4Intermediate Member
- Join Date
- May 2020
- Location
- ACT
- Posts
- 27
Thanks Kryn,
I used 1018 RHS I think it was 75 X 35 5mm wall. If I did it again I'd probably use 4140 for a bit better tensile strength, I did put a bit of a bend in one once (trying to get under a log that I reckon weighed in at about 600kg!). But that really was abuse on my part.
-
19th Jun 2020, 02:05 AM #5Intermediate Member
- Join Date
- May 2020
- Location
- ACT
- Posts
- 27
Thanks Steve,
I used 1018 RHS, I think it was 75 X 35 5mm wall. I'd probably use a similar section again but go for 4130 as I did manage to bend one fork at one stage due to abuse on my part. I was lifting a massively heavy redgum log out of a creek bed and tried a repositioning lift on a single fork. It was a minor bend but annoying to fix. At the right angle intersection I butt welded the RHS and placed a 6mm L bracket (with a 50mm radius) along each side of the RHS. The bracket probably extended 100mm each direction.
-
19th Jun 2020, 02:20 AM #6Intermediate Member
- Join Date
- May 2020
- Location
- ACT
- Posts
- 27
A Couple of shots, one showing the fork right angle intersection, the other showing the firewood laden crates I used to move around the property with the forks. These crates weighed in at around 430-450kg each. Typically we were moving them around on pretty bumpy ground so they didn't have an easy time of it!
IMG_5369.pngIMG_5368.png
-
19th Jun 2020, 12:59 PM #7Most Valued Member
- Join Date
- Nov 2017
- Location
- Geelong, Australia
- Age
- 57
- Posts
- 2,666
Out of interest, did the fork bend at the joint, or on either the horizontal or vertical straight section?
The extension tynes/slippers they have at work are about 6mm thick, and fabricated from an upside down C section with flat welded across the open side (the bottom when in use). Not sure of the material but likely some alloy steel as it looks and machines like that.
I've got the remains of one here that was scrapped after one of the forkies managed to jam a lump of pallet timber up inside that couldn't be extracted
Only mentioning the construction method as it allows for different thickness top and bottom, albeit with a bit more welding required. Also allows easy access to the inside of the section prior to welding up the open side if you wanted to add additional material at a stress point.
More design thought and fabrication, but stronger product for same or less weight.
I'm pretty sure Duragal is 450Mpa so that might be a reasonable option if you did need something slightly stronger in the future - without going to full on 4130 etc.
Damn nice job you've done with those ones though!!
Steve
-
19th Jun 2020, 08:23 PM #8Intermediate Member
- Join Date
- May 2020
- Location
- ACT
- Posts
- 27
Thanks Steve, That sounds like a really good option. I didn't realise that Duragal had a better tensile strength but that makes sense through. I made the uprights at the ends with Duragal RHS (150 x 50 I think). I made the tapered shape by cutting a 'cap' off the edge of each section and removing a wedge shape from the sides (with the plasma), I then welded each edge section back on the the reshaped RHS. When I took the 'caps' off the section opened up madly! Heaps of stress in Druagal RHS i found out!
The fork that bent (about 5 degrees) actually took quite a bit to do so, it had about 1.3 ton's of moving tractor behind it and was lifting at the same time! It bent about 150mm out from the edge of the L bracket on the horizontal section. I ended up straitening it in the press and never had another issue. I think I was a bit lazy that day and really should have pulled the log out of the creek with a drag chain first. We are talking redgum about 500mm diameter and about 3m long!
Craig.
Similar Threads
-
Tractor Repairs
By Oldneweng in forum METALWORK GENERALReplies: 10Last Post: 5th Sep 2016, 08:11 PM -
Steel wheel Fordson tractor
By bob ward in forum ANTIQUE AND VINTAGE MACHINERYReplies: 2Last Post: 10th Jul 2016, 11:31 PM -
Tractor Carrier
By Styx in forum TRAILERS & OTHER FABRICATED STUFFReplies: 45Last Post: 18th Nov 2012, 07:25 AM -
Andre's homebuilt tractor
By welder in forum TRAILERS & OTHER FABRICATED STUFFReplies: 3Last Post: 11th Apr 2010, 09:36 AM -
Andre's articulted tractor build
By welder in forum TRAILERS & OTHER FABRICATED STUFFReplies: 4Last Post: 29th May 2009, 04:47 PM