Needs Pictures: 0
Results 16 to 18 of 18
Thread: Aluminium Caravan Question
-
6th Dec 2018, 11:11 PM #16Most Valued Member
- Join Date
- May 2011
- Location
- Murray Bridge S Aust.
- Age
- 71
- Posts
- 5,959
Had a gander at the aluminium plant trailer at work as to how the suspension and coupling is attached. The coupling is attached with HT bolts, and the suspension is welded to 150 X 75 X 10 angle, then that is bolted to the aluminium chassis, which is 200 X 75 Channel. The channel is rolled into a curve, similar to the link below.
Aluminium Plant Trailers | Sureweld
The caravan chassis would have outriggers to support the floor and composite sides, as per the image below.caravan chassis 1.jpgcaravan chassis 2.jpg
Have found an image as to how composite caravans are attached to the framing. Sealant would be used on all the joints.
Composite.jpg
Hope this helps.
KrynTo grow old is mandatory, growing up is optional.
-
7th Dec 2018, 12:39 PM #17Most Valued Member
- Join Date
- Nov 2017
- Location
- Geelong, Australia
- Age
- 57
- Posts
- 2,672
When I was building the dinghies one of the guys owned a chandlery, and we were just using common Epiglass resins.
For specialist bonding the best bet is probably to get hold of the sales/tech reps for major manufacturers or a specialist composite supplier/distributor and see what they recommend for your particular purpose. Just keep in mind that the more specialised the product, the more expensive it will be, and also the more specific the preparation and application will be. Personally I'd be looking at appropriate design so you don't need to go too hi-tech.
Something to keep in mind is to allow for flex/movement where appropriate. Composite panel structures are very rigid. If you attach one solidly to a chassis structure that is designed to flex you will introduce a stress point at the join.
Steve
-
7th Dec 2018, 01:01 PM #18Senior Member
- Join Date
- Dec 2013
- Location
- Sydney
- Posts
- 201
West System epoxies are available at chandlers and fibreglass suppliers. West make an excellent range of general epoxy resins. But you wouldn't need to use epoxy unless you are specifically bonding a composite structure to aluminium. Polyester resin (the stinky stuff that everyone associates with fibreglass work) would be quite OK for making up and joining the composite panels, and polyester is much cheaper and easier to use that epoxy laminating resin.
I'd go so far as to suggest that even if the shell needs to be bonded to an aluminium frame, that polyester resin and glass over a suitable foam core would be the way to go, and to solve the bonding problem by choosing a suitable glue that bonds polyester/fibreglass to aluminium (some sort of Sikaflex, or builders adhesive?). Or design a suitable bolted fixing.
Steve is right to warn of the massive stiffness that a composite box structure will exhibit. But that's a good thing to have, and is a design benefit. You just need to design the frame and fixings accordingly.
Graham.
Similar Threads
-
question re aluminium grade
By texx in forum METALWORK GENERALReplies: 6Last Post: 18th Sep 2018, 10:26 PM -
Drilling Aluminium Question
By cava in forum METALWORK GENERALReplies: 25Last Post: 22nd Feb 2017, 09:08 AM -
Milling Aluminium - A Question
By Anorak Bob in forum METALWORK GENERALReplies: 8Last Post: 9th Jun 2016, 08:34 PM -
aluminium tig question
By kelack in forum WELDINGReplies: 9Last Post: 14th Oct 2014, 09:49 PM -
welding gas for aluminium question
By northerncat in forum WELDINGReplies: 3Last Post: 14th May 2009, 02:00 PM