Page 2 of 2 FirstFirst 12
Results 16 to 18 of 18
  1. #16
    Join Date
    May 2011
    Location
    Murray Bridge S Aust.
    Age
    71
    Posts
    5,959

    Default

    Had a gander at the aluminium plant trailer at work as to how the suspension and coupling is attached. The coupling is attached with HT bolts, and the suspension is welded to 150 X 75 X 10 angle, then that is bolted to the aluminium chassis, which is 200 X 75 Channel. The channel is rolled into a curve, similar to the link below.
    Aluminium Plant Trailers | Sureweld
    The caravan chassis would have outriggers to support the floor and composite sides, as per the image below.caravan chassis 1.jpgcaravan chassis 2.jpg
    Have found an image as to how composite caravans are attached to the framing. Sealant would be used on all the joints.
    Composite.jpg
    Hope this helps.
    Kryn
    To grow old is mandatory, growing up is optional.

  2. #17
    Join Date
    Nov 2017
    Location
    Geelong, Australia
    Age
    57
    Posts
    2,672

    Default

    Quote Originally Posted by cava View Post
    Thanks Steve.

    I was thinking of a composite body, but unsure of how to secure it to a trussed design. Where do you get the special epoxies from?

    George
    When I was building the dinghies one of the guys owned a chandlery, and we were just using common Epiglass resins.
    For specialist bonding the best bet is probably to get hold of the sales/tech reps for major manufacturers or a specialist composite supplier/distributor and see what they recommend for your particular purpose. Just keep in mind that the more specialised the product, the more expensive it will be, and also the more specific the preparation and application will be. Personally I'd be looking at appropriate design so you don't need to go too hi-tech.

    Something to keep in mind is to allow for flex/movement where appropriate. Composite panel structures are very rigid. If you attach one solidly to a chassis structure that is designed to flex you will introduce a stress point at the join.

    Steve

  3. #18
    Join Date
    Dec 2013
    Location
    Sydney
    Posts
    201

    Default

    West System epoxies are available at chandlers and fibreglass suppliers. West make an excellent range of general epoxy resins. But you wouldn't need to use epoxy unless you are specifically bonding a composite structure to aluminium. Polyester resin (the stinky stuff that everyone associates with fibreglass work) would be quite OK for making up and joining the composite panels, and polyester is much cheaper and easier to use that epoxy laminating resin.

    I'd go so far as to suggest that even if the shell needs to be bonded to an aluminium frame, that polyester resin and glass over a suitable foam core would be the way to go, and to solve the bonding problem by choosing a suitable glue that bonds polyester/fibreglass to aluminium (some sort of Sikaflex, or builders adhesive?). Or design a suitable bolted fixing.

    Steve is right to warn of the massive stiffness that a composite box structure will exhibit. But that's a good thing to have, and is a design benefit. You just need to design the frame and fixings accordingly.

    Graham.

Page 2 of 2 FirstFirst 12

Similar Threads

  1. question re aluminium grade
    By texx in forum METALWORK GENERAL
    Replies: 6
    Last Post: 18th Sep 2018, 10:26 PM
  2. Drilling Aluminium Question
    By cava in forum METALWORK GENERAL
    Replies: 25
    Last Post: 22nd Feb 2017, 09:08 AM
  3. Milling Aluminium - A Question
    By Anorak Bob in forum METALWORK GENERAL
    Replies: 8
    Last Post: 9th Jun 2016, 08:34 PM
  4. aluminium tig question
    By kelack in forum WELDING
    Replies: 9
    Last Post: 14th Oct 2014, 09:49 PM
  5. welding gas for aluminium question
    By northerncat in forum WELDING
    Replies: 3
    Last Post: 14th May 2009, 02:00 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •