Originally Posted by
gazza2009au
Extension lead is about 20 years old i've had it for 20 years.. its 15amp lead but the plugs were changed to 10amp by my brother who i got it off 20 years ago
I run the cable mostly uncoiled but there may be a knot or two, the power was fine one day than the next i had to up the amps i just assumed with the amount of rods i went thru (at lease 20 rods) the machine was just broken in and settled down a little but that is just my thinking im a mechanic not an electrician