31st Aug 2007, 09:16 PM #1
Cover lens spares for Tecmen AD helmet
Hi everyone,
By now many of us who have the Tecmen brand helmets may have used up the clear plastic cover lens and spare.
Trying to source a replacement lens was a PITA as the potential candidates at the local welding supply were too big ,too small, too thick and too expensive.
I took my old cover lens to a plastics dealer,in my case Consolidated Plastics in Mackay.They were able to provide a sheet of poycarbonate exactly the same thickness as the original Tecmen lens.
For $5 I was able to purchase a sheet which provided 12 replacement lenses.
Hopefully you may have the same success with your local plastics dealer..
Grahame
-
1st Sep 2007, 06:30 PM #2Diamond Member
- Join Date
- Aug 2006
- Location
- Melbourne
- Posts
- 1,106
I ended up just using standard cig lenses and made up a rubber strip about 6mm or so to fill the missing space.