    Default My welding skills are ... inferior

    I am not a welder.
    Against all odds I try to get a nice bead on thin material with an old stick welding machine.
    What could possibly go wrong?

    Shot2.jpg

    I present my questionable skills in this video

  2. #2
    Join Date
    Dec 2005
    Location
    South Australia
    Posts
    1,658

    Default

    Need to turn you amps down, plus your electrode angle is incorrect, that type of join is not the best to start out on, you just need more practice, find some scrap and get your basic technique right doing simple butt welds.

  3. #3
    Join Date
    Nov 2019
    Location
    Brisbane
    Age
    69
    Posts
    452

    Default Arc welding

    Hello Finno.
    If your using an old transformer welder ( heavy ) that could be part of the problem. They are AC and low open circuit voltage. Modern electrodes are formulated for DC and high voltage. A good web site to visit is weld.com A Canadian welding school with video thru the lens.
    Another tip is clean the metal and don't try to weld air gaps.
    Regards
    BC

  4. #4
    Join Date
    Apr 2018
    Location
    Perth
    Posts
    168

    Default

    To get practice of laying down a nice bead, dont try to weld 2 pieces together.
    Start by practicing on a thick piece of clean steel and get your beads looking right. play around with current and angles and speed until the weld looks ok then try joining metal together.
    A butt joint is hard to do without blowing holes in it, start with lap joints .

Similar Threads

  1. Some welding and fab skills to aspire to
    By Grahame Collins in forum WELDING
    Replies: 3
    Last Post: 11th Feb 2022, 08:05 PM
  2. Gunsmithing skills on display 1969
    By morrisman in forum GUNSMITHING
    Replies: 8
    Last Post: 22nd Jan 2022, 10:44 PM
  3. What skills and tools do i need to build this?
    By stonedpirate in forum METALWORK GENERAL
    Replies: 27
    Last Post: 16th Apr 2015, 08:49 AM
  4. Having Welding Skills Assessed?
    By ARock in forum WELDING
    Replies: 1
    Last Post: 23rd Apr 2009, 07:24 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •