10th Nov 2021, 08:41 PM #16Most Valued Member
- Join Date
- Nov 2008
- Location
- North Brisbane. Qld. Australia
- Age
- 70
- Posts
- 1,514
Can someone explain to me the point of welding a pinch bar, to a tow bar tongue, for the purpose of testing a weld. I would assume the pinch bar is forged and probably a Chinese forging and shouldn't be welded anyway, so what does breaking it prove?
Nev.
-
10th Nov 2021, 10:14 PM #17Intermediate Member
- Join Date
- May 2009
- Location
- melb
- Posts
- 25
Would be much appreciated to get an opinion on my question. I know this is a forum of people who enjoy working with metal and discussion is great but would love to hear what you guys think about those beads if you can draw any conclusions here. I could keep on trialling and erroring but if I can limit wastage with advice that would be great
-
11th Nov 2021, 09:34 PM #18
Enough Gentlemen.
Lets remember we are all here responding to a new members post for assistance with setting his Unimig Viper 185 MIG Welding machine.
What we have seen is hardly a good first impression for him, is it?
Lets keep our posts polite and civil OK.
Querty.
A couple of issues to sort out before we begin. DO you have Unimig Viper 185 model that incorporates a digital amperage and voltage display?
Like this?
Unimig Viper 185.jpg
What will be really helpful is to record the numbers displayed for each of those sample beads ( hint! next time around I would make them longer say 50 mm minimum length)
A question for you, is what electrode wire stickout were you using and were you pulling or pushing the arc? Stickout is how much wire (distance ) between contact tip and the work( or arc) when you are welding.
I'll comeback later with more when you have given me a have a better idea of how you set up your welder before running those beads.
For the moment I would not worry about welding 10mm flat bar, lets improve the bead appearance first.
Cheers
Grahame
-
12th Nov 2021, 07:03 PM #19
There are at least 3 variations to the above that I can think of;
1. A tee piece,the 2. 5 mm thickness being perpendicular to the 10mm.
2. A butt configuration with the 2.5 mm flush with and parallel to 10 mm flat.
3. As an overlap where the 2.5 mm thickness is laid over the top and the 2.5mm edge is welded to the 10 mm
Yes if you have a stick electrode function this is possible, but some position choices are more difficult than others.
Again, that is best left until you sort out your current challenge of setting up the wire speeds to a better standard.
Grahame
-
13th Nov 2021, 08:15 AM #20Intermediate Member
- Join Date
- May 2009
- Location
- melb
- Posts
- 25
-
13th Nov 2021, 02:14 PM #21Diamond Member
- Join Date
- Jun 2010
- Location
- Canberra
- Posts
- 1,322
I'll have a go - although completely unqualified, I've owned a Unimig 165 inverter for 10+ years and have, on occasion, welded 10mm+ with it, but that's multiple passes on a bevelled joint with a root gap.
Of the beads you posted, 14 looks the best in terms of fully wetted edges, and it's really the edges you should be looking at while welding. If you're pushing, you want the leading edge to be chewing out the base metal, and then the weld pool filling back in and washing out fully to the sides.
Australian pro welders tend to get angry about any kind of torch movement, whereas yanks are all about making their patterns. I certainly find that some kind of movement helps me to maintain a consistent weld speed, as well as making sure the weld pool is hitting all the right edges.
-
14th Nov 2021, 01:09 PM #22
Hi Querty.
Rather than just talk about how to set your machine to weld a specific metal thickness it is more desirable to look at how to recognise those characteristics of a good sound Mig weld bead and the conditions which allow it to be formed.
We will address what can be seen with the naked eye first - often referred to as a visual inspection. The purpose is to identify Mig weld bead defects and to learn what undesirable action causes those particular defects.
The characteristics of a good MIG bead.
- A uniform width through out the length of the bead.
- A uniform height throughout the length of the bead
- A uniform cross sectional profile throughout the length of the bead
- An absence of porosity and cavities
- An absence of craters
- An absence of undercut at the bead toes (the edges) throughout the length of the bead
- An absence of excessive spatter
Conditions that form Mig weld bead characteristics
- A uniform width through out the length of the bead.- Consistent travel speed, consistent stick out
- A uniform height throughout the length of the bead - Consistent travel speed, consistent stick out
- A uniform cross sectional profile throughout the length of the bead Consistent travel speed, consistent stick out
- An absence of porosity Adequate shielding gas, clean gas nozzle shroud, no leaks in gas line or has shroud,No foreign materials on weld surface
- An absence of craters Pausing to fill crater on completion of bead or backstep weld arc to fill crater on restart of incomplete bead
- An absence of undercut at the bead toes (the edges) throughout the length of the bead. Amperage setting, travel speed and weld angle not excessive
- An absence of excessive spatter Travel speed not excessive, amperage (wire speed setting) not excessive
Regarding the push/[pull arguments Lincoln Electric has a great set of guidelines which Mig welders might find extremely useful to save.
https://www.lincolnelectric.com/asse...L-50/c4200.pdf
You will naturally have questions,so I'll pause here and wait until you read and digest the above.
Cheers
Grahame
-
24th Feb 2022, 04:17 PM #23Banned
- Join Date
- Mar 2012
- Location
- Sunshine Coast, QLD
- Posts
- 9
As an absolute rank amateur ...
To my way of thinking welding 10mm anything with a relatively inexpensive welder sets off alarm bells. People like me buy something like a Unimig Viper 185 (hey, I did) to do odd jobs and may one day progress to bigger stuff, with more skill, along with more sophisticated equipment. If we're not talking BBQ plates and are actually talking about things that could be under significant load, I'd be very worried.
So ...
Would personally weld a BBQ plate or a veranda support, maybe a fence bracket or a base for a post supporting a solar panel? ... Absolutely YES.
Would I weld a tow bar or a car's suspension component? NO.
With any do it yourself activity you need to ask yourself what could go wrong if it breaks and in the situation where there's a high risk PLEASE THINK TWICE
Similar Threads
-
Parting Off and Sutton's Viper Cutting Fluid
By bwal74 in forum METALWORK GENERALReplies: 3Last Post: 21st Mar 2021, 06:16 PM -
Uni-Mig Viper 200DC TIG/MMA Welder - KUMJRVT200P
By Mark_C_86 in forum WELDINGReplies: 5Last Post: 27th Apr 2020, 01:27 PM -
Viper 182 Unimig Any feed back ?
By getsquigs in forum WELDINGReplies: 3Last Post: 23rd Apr 2016, 09:54 PM -
Laser cut 10mm steel pricing?
By DoctorWu in forum METALWORK GENERALReplies: 6Last Post: 19th Feb 2015, 09:34 PM -
bending 10mm round bar
By Dusty Wheels in forum METALWORK GENERALReplies: 24Last Post: 22nd Aug 2007, 08:52 PM