17th Sep 2021, 02:12 PM #1New Member
- Join Date
- May 2019
- Location
- Albury
- Posts
- 3
stainless exhaust tig welding
Hi to all,
I am fabricating a marine exhaust system from 1.6 mm stainless tubing and have welded one joint using argon purging. I now have to marry the tube to a reducer and the next weld will coincide with the first. will I need to purge the existing weld a second time?
Any ideas will be greatly appreciated.
-
17th Sep 2021, 03:38 PM #2
Hi Q585,
Welcome to the MetalWork Forums,
I am sure there many welders and like minded people here who will welcome you and offer their input and experience.
To navigate our Forums click on the FORUM box at the LH top of the page.
A drop down menu will appear and click on FORUM HOME which will give you a scroll down page with all of our various sub forums and other helpful things on
Our forum rules, the TOU's are on top and the rest is the sub Forums and help pages that make up our forum package.Please make sure to read through them.
cheers
Grahame
-
17th Sep 2021, 03:48 PM #3
No purge needed for the original beads.
The purge operates when the bead being welded is still semi molten and cooling.
The purge gas protects the cooling bead from the ravages of oxidisation.
Yes you will still require a purge medium otherwise your bead internal bead surface( being welded) will oxidise if not protected.
To avoid having to purge large areas of the tube, a sneaky trick is to block off (areas not needed ) with toilet tissue.
As its made not to block pipes ,the tissue can be flushed out later with copious amounts of water.
Cheers
Grahame
-
17th Sep 2021, 05:16 PM #4Senior Member
- Join Date
- May 2013
- Location
- Rockhampton, QLD
- Age
- 68
- Posts
- 456
Welcome to the forum.
-
21st Sep 2021, 04:26 PM #5New Member
- Join Date
- May 2019
- Location
- Albury
- Posts
- 3
Stainless exhaust welding
Hi Grahame,
Thanks for your response, and the advice. The toilet paper idea is a good trick to know!
I got the welds done after a bit of mucking around with my custom made purging set up, but it all turned out ok.
Thanks again. SteveJ.
-
21st Sep 2021, 04:42 PM #6New Member
- Join Date
- May 2019
- Location
- Albury
- Posts
- 3
New member welcome
Similar Threads
-
Need some advice TIG welding used stainless exhaust
By gazza2009au in forum WELDINGReplies: 10Last Post: 2nd Aug 2015, 08:46 PM -
MIG welding a cast iron exhaust manifold.
By aametalmaster in forum WELDINGReplies: 4Last Post: 19th Feb 2012, 11:50 PM -
Welding stainless
By mcchaddy in forum WELDINGReplies: 14Last Post: 20th Apr 2011, 09:08 AM -
MIG Welding Stainless
By Bad Fruit in forum WELDINGReplies: 4Last Post: 30th Apr 2010, 06:12 PM -
Welding thin Stainless
By pipeclay in forum WELDINGReplies: 15Last Post: 12th Jun 2009, 04:37 PM