Alum TIG Filler
I have some cracks in unknown aluminium tube to weld up.
I haven't TIG welded Alum for 30ish years.
I purchased some ER5356, partly because I remember almost nothing about this sort of thing and party because the guy I buy my TIG stuff from currently has no 4053.
Given my "some what" lacking experience.
Is one likely to be better than the other?(or unanswerable given the unknown alloy)
Is someone with my level of experience going to notice a difference?
I have heard it said you never know what you are going to get tig welding unknown alum until you light the torch.
-
27th Jul 2021, 07:59 AM #2
4043 for extrusions. IIRC it has a higher silicone content.
5356 for castings (higher magnesium), and the standard 3000-6000 series materials.
-
27th Jul 2021, 04:51 PM #3Diamond Member
- Join Date
- Aug 2006
- Location
- Melbourne
- Posts
- 1,105
When I was pulse migging aluminium I was using 5356 for everything, extrusions, castings, plate and pipe material.
Sent from my SM-G935F using Tapatalk
-
27th Jul 2021, 06:13 PM #4Most Valued Member
- Join Date
- Aug 2009
- Location
- Sydney, NSW, Australia
- Posts
- 1,836
A good tip the guys from thisforum have given meis clean the oxide off the job with astainless brush and use stainless steel wool to clean the oxide off the tig filler rods, after this the aluminum will melt like butter
-
27th Jul 2021, 10:47 PM #5Most Valued Member
- Join Date
- Jul 2010
- Location
- Melbourne
- Posts
- 9,088
Thank you gents,
I'll get some when they are back in stock.
I have a pulse TIG, but please don't confuse that with being able to use it.
Will find something to practice on.
Bunnings has Acetone and S/S brushes.
These do to clean the filler?
https://shop.coles.com.au/a/national...l-scourers-3pk
-
28th Jul 2021, 08:31 AM #6Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,542
Yes, those will do to clean the filler, although I find that if the filler has been kept away from dust and moisture then usually a wipe with acetone is enough. It's the materials you are joining that need the serious attention.
As for filler, while certain fillers are better for particular materials, I use 5356 for all the Al welding I do without ill effects. Unless you are doing aerospace work where the metallurgical properties are critical or volumes of parts where the cost of having several types of filler on the shelf is not an imposition, Al filler choice is not life or death where one will work and the other causes serious problems.
Michael
-
28th Jul 2021, 09:16 AM #7Member
- Join Date
- May 2021
- Location
- Sunshine Coast QLD
- Posts
- 62
I have to weld a crack in a Bike swingarm (1981 Suzuki RM125X)
I consulted a number of expert forums.
Got similar advice to what’s on this thread.
Basically- difficult to determine what grade of Al it is.
5356 should do the job. (One guy had experience with it not working on one swingarm - the filler fell out after anodising!!)
Clean everything.
Pre heat it a bit.
-
21st Aug 2021, 09:40 PM #8Most Valued Member
- Join Date
- Jul 2010
- Location
- Melbourne
- Posts
- 9,088
All the stars aligned and I got some "welding" done. 2 inches is really enough to learn much though.
Its more "blobs melted together" than welds.
It's 1mm alum, I started at 10A and left it there.
If nothing else the cleaning seems to have worked.
-
21st Aug 2021, 10:58 PM #9Member
- Join Date
- May 2021
- Location
- Sunshine Coast QLD
- Posts
- 62
I’ve been practicing.
Been getting a few “jobs” since Ive been claiming to be able to “weld aluminium”.
-
22nd Aug 2021, 10:26 AM #10Diamond Member
- Join Date
- Oct 2008
- Location
- N.W.Tasmania
- Posts
- 1,407
Similar Threads
-
Cheap alum welding
By kenny_10 in forum WELDINGReplies: 4Last Post: 3rd Sep 2018, 05:35 PM -
Heat from arc welding - alum mould - what will happen?
By newbyangler in forum WELDINGReplies: 4Last Post: 15th Jun 2016, 01:32 PM -
Filler rod size for TIG
By Michael G in forum WELDINGReplies: 22Last Post: 19th Jul 2012, 12:13 AM -
Welder to mig steel and alum
By KWD in forum WELDINGReplies: 8Last Post: 20th Dec 2011, 08:32 PM -
Cutting Alum Round Bar
By Bidgee in forum METALWORK GENERALReplies: 6Last Post: 5th May 2010, 06:54 PM