CIG Transmig
Hi all new to this forum.
I have acquired a CIG Transmig from mid 1980’s.
I do very little welding and this is a big unit and it is not worth the cost of the argon bottle just to have it sitting there taking up space.
After some advice. Will is work with gasless wire?
should I move it on and get a smaller more modern unit?
Is this old unit worth any money or should I look to give it away ?
cheers
-
22nd Jul 2021, 08:31 PM #2Diamond Member
- Join Date
- Aug 2006
- Location
- Melbourne
- Posts
- 1,106
-
23rd Jul 2021, 07:54 AM #3Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,563
Are you aware that while the old cylinder rental schemes are still around, people like Bunnings will sell you just the gas with the cylinder secured by a refundable deposit? A D size is from memory $200 deposit. Some have argued against the scheme in the past, saying that the amount of interest on the $200 they lose by having the money tied up is excessive but I find it a far better proposition than quarterly rental, especially for irregular use.
Michael
-
24th Jul 2021, 12:06 PM #4Most Valued Member
- Join Date
- Nov 2007
- Location
- melbourne australia
- Posts
- 3,228
-
24th Jul 2021, 04:49 PM #5
Welcome to the forums.
There were a whole bunch of Transmig models. A pic of your machine will be handy.
The model I am thinking you might have is the squarish box shaped body steel in sheet metal. The was the plain straight polarity (electrode negative ) -therefore gas shielded solid wire.
The other Transmig that comes to mind for gasless wire, the Transmig195 Rural pak had reversible polarity to allow such use.
Both were rugged well made machines which I suspect were re badged Miller Machines who had a tie up with CIG around that time.
Long story short, unless you have 195 Transmig Rural pak there no gasless wire capability.
Grahame
Similar Threads
-
Transmig 172
By russ57 in forum WELDINGReplies: 9Last Post: 25th Oct 2020, 07:01 AM -
CIG Transmig 200
By Sterob in forum METALWORK GENERALReplies: 5Last Post: 20th Jul 2020, 01:32 PM -
Transmig 195 gun
By bwah in forum WELDINGReplies: 6Last Post: 30th Oct 2014, 03:46 PM -
Transmig 135
By ijump in forum WELDINGReplies: 4Last Post: 17th Mar 2011, 08:21 PM -
CIG transmig 150
By timbo123 in forum WELDINGReplies: 8Last Post: 31st Jul 2006, 10:45 AM