    Default Everlast Equipment or is it Neverlast?

    Looking around for a decent 60 amp plasma. Seems to me in this size which is about the biggest single phase plasma cutter you can get the choice is an Everlast or a Cigweld.

    The Everlast has a significantly better duty cycle then the cigweld and is quite heavier in weight.

    Anyone have any experience with Everlast? It seems the local dealer has absolutely no stock of anything Everlast though https://www.everlastwelders.com.au/collections/welders

    Anyone know of any other options for decent 60 amp plasma cutters?
    Gold, the colour of choice for the discerning person.

  2. #2
    Join Date
    Oct 2008
    Location
    N.W.Tasmania
    Posts
    1,407

    Default

    Absolutely no experience with them Richard, but as I recall several big names in the YouTube creator Community, or at least the U.S. based ones have Everlast gear and seem to like it. (Adam Booth for one) Possibly they have a similar reputation to the TokenTools gear here in Australia. I find it remarkable that the Australian agent has no gear at all, perhaps Covid will be what they blame for their situation.

  3. #3
    Join Date
    Dec 2005
    Location
    South Australia
    Posts
    1,658

    Default

    Don't take any recommendation from Adam Booth, his channel is just paid advertising these days. A mate in Andamooka has Everlast MIG it was not cheap around $6000, he is very happy with it
    has been going for three years

  4. #4
    Join Date
    Nov 2019
    Location
    Brisbane
    Age
    69
    Posts
    452

    Default Plasma cutter

    Hello again to all.
    Single phase plasma cutters can be limited by the power available. At 60A output it might need 25A from the wall. I sell 45A 240V plasma cutters with confidence that they will work well. You have a good choice but I have had a good run with the Razor 45. Spares are at a good price as well. You may get a bundle deal this month with an air filter.
    Regards
    BC

  5. #5
    Join Date
    Aug 2008
    Location
    near Rockhampton
    Posts
    6,218

    Default

    Quote Originally Posted by steamloco1954 View Post
    Hello again to all.
    Single phase plasma cutters can be limited by the power available. At 60A output it might need 25A from the wall. I sell 45A 240V plasma cutters with confidence that they will work well. You have a good choice but I have had a good run with the Razor 45. Spares are at a good price as well. You may get a bundle deal this month with an air filter.
    Regards
    BC
    I have 32 amp sockets at my disposal, and ideally I would get an 80 amp but they do not import 80 amp 240V plasma cutters and they would need a 63 amp socket, which I now see are available in Australia being some European standard (they go up to and over 100 amp 240v sockets and plugs)

    I already have a Razorcut 45 which mine actually puts out 50 amps, but it is just not cutting it for my needs these days. Even for a razorcut 45 you cannot run them successfully off a 15 amp socket at full output. Mine just keeps flicking out the 20 amp use in the switchboard.
    Gold, the colour of choice for the discerning person.

  6. #6
    Join Date
    Oct 2012
    Location
    Wallerawang NSW
    Posts
    28

    Default Everlast Quality

    I have an Everlast TIG Welder - It has all the bells and whistles and the quality is wonderful. The cables, clamps hand pieces are all top quality and it works exactly as it should. I can't recommend them enough.
    Steve

  7. #7
    Join Date
    Sep 2008
    Location
    lillimur
    Posts
    86

  8. #8
    Join Date
    Oct 2012
    Location
    Wallerawang NSW
    Posts
    28

    Default

    Quote Originally Posted by rascal View Post
    I was speaking of the brand in general terms from my experience.

  9. #9
    Join Date
    Nov 2004
    Location
    Bungama SA
    Age
    52
    Posts
    960

    Default

    My Everlast machine is still going fine been using it for a few years now.

    I dont think their quality is a problem and I had no trouble with the Aust dealer
    ....................................................................

  10. #10
    Join Date
    Aug 2008
    Location
    near Rockhampton
    Posts
    6,218

    Default

    I am going to get one think. Just waiting on stock. It seems they are going to be as good as the brands like Unimig which I think are sort of middle of the road in quality and priced along those lines.
    Gold, the colour of choice for the discerning person.

Similar Threads

  1. Ahh bugger my misfortune.. First model Everlast AC/DC Tig FaceBook NSW
    By gazza2009au in forum EBAY, GUMTREE, and other off forum sales sites
    Replies: 3
    Last Post: 27th Dec 2017, 08:34 PM
  2. I dig My Everlast 200T Tig
    By WillyInBris in forum WELDING
    Replies: 7
    Last Post: 9th Nov 2015, 06:37 PM
  3. Everlast Welder
    By awpy in forum WELDING
    Replies: 10
    Last Post: 11th Feb 2015, 06:32 PM
  4. Tokentools Alusync vs Everlast PowerTig
    By C110GTR in forum WELDING
    Replies: 11
    Last Post: 28th Jun 2012, 10:19 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •