3rd Feb 2021, 10:59 AM #1New Member
- Join Date
- Feb 2021
- Location
- sydney australia
- Age
- 46
- Posts
- 2
what is this coated with?
hi all. im new here, and new to mig welding. many years with a stick but wanna learn mig. something im trying to work out is what this is coated with. i have this piec of old try i want to practice with, but it has some kind of coating on it that i cant see.
ive tried hydrochloride acid, sulphuric acid, acetone, thinners, petrol, blowtorch. nothing removes it.
ive noticed that a few other pieces of scrap seem the same somehow. quite simply, i cant trike an arc on them.
what is this coating and how do i remove it?
-
3rd Feb 2021, 11:23 AM #2Intermediate Member
- Join Date
- Oct 2012
- Location
- Wallerawang NSW
- Posts
- 28
-
3rd Feb 2021, 01:02 PM #3Most Valued Member
- Join Date
- Jul 2016
- Location
- Melbourne
- Age
- 35
- Posts
- 1,522
Itll be anodised. Id just buy some sheet or bar of a known grade.
Sent from my SM-G973F using Tapatalk
-
3rd Feb 2021, 01:57 PM #4Member: Blue and white apron brigade
- Join Date
- Feb 2006
- Location
- Perth
- Posts
- 7,189
Quite few things will remove anodising but unfortunately may also attack the Al underneath - caustic soda base drain cleaner for instance will do that.
There is a product called "Greased Lightning" which is commonly used to strip anodising off small parts but its MSDS says itsa 10% solution of caustic soda plus glycol ether and a surfactant. It claims not to affect the Al but it does say not to leave parts in for too long.
Anodizing can be dissolved without affecting the underlaying Al using a dilute solution of phosphoric and chromic acid. The latter is nasty stuff - best kept away from.
-
3rd Feb 2021, 02:50 PM #5Most Valued Member
- Join Date
- Nov 2017
- Location
- Geelong, Australia
- Age
- 57
- Posts
- 2,671
Is there a reason you can't remove it mechanically?
Steve
-
3rd Feb 2021, 04:19 PM #6New Member
- Join Date
- Feb 2021
- Location
- sydney australia
- Age
- 46
- Posts
- 2
thanks for your replies guys.
to answer questions 1 by 1.
theres no reason i cant remove it mechanically, just time and work thats all.but for the sake of learning id also like to learn what it is, how do i tell, and other possible ways to remove it.
i will check out the phosphoric and chromic acid.
after playing around with it, i realized if i grind 1 piece, i can run from that as long as i dont try to flow too fast. i cant start an arc on a fresh clean piece,but as long as i weld from a previous weld im right. the way that it pools is slightly different, so a matter of playing with the settings.
-
3rd Feb 2021, 05:32 PM #7
Hi jfoldbar,
Welcome to the MetalWork Forums.
To help you explore the other areas of our forum here's a guide on to to navigate our Forum and find all the interesting places.
Goto the FORUM box in the top left hand cnr of the page and click the down arrow. This will bring up a pull down menu that has Forum Home at the top
Click Forum Home which will present a scroll down page.
Our rules,the Terms of Service are right at the top ,we encourage you to read them.
Below that are all the various areas and sub forums that make up out MetalWork forums.
Welcome
Grahame
-
3rd Feb 2021, 06:45 PM #8Senior Member
- Join Date
- May 2013
- Location
- Rockhampton, QLD
- Age
- 68
- Posts
- 455
Welcome to the forum.
Similar Threads
-
Coated Indexable Inserts For Sale
By Col2310 in forum METALWORK - Machinery, Equipment, MARKETReplies: 1Last Post: 11th Mar 2019, 12:53 PM -
Sharpening coated end mills
By newmanwoodlands in forum METALWORK GENERALReplies: 32Last Post: 8th Feb 2018, 09:54 PM -
Nippon Coated Abrasives
By ozhunter in forum METALWORK GENERALReplies: 4Last Post: 4th Oct 2012, 10:07 PM -
Can polished Stainless-Steel be powder-coated?...