Results 31 to 38 of 38
Thread: Cheapest MIG that'll do the job?
-
2nd Jan 2021, 08:30 PM #31Most Valued Member
- Join Date
- Nov 2007
- Location
- melbourne australia
- Posts
- 3,228
Here's the duty cycle curve of the Bossweld S180 stick welder if anyone's interested.
Chris
-
3rd Jan 2021, 08:39 AM #32Diamond Member
- Join Date
- Oct 2011
- Location
- Sydney, NSW
- Posts
- 1,249
IRT TAFE, I wanted to do a metal fabrication course this year. The only TAFE in the Sydney Metro area is Ultimo TAFE. That's the only TAFE for all engineering type TAFE short courses in Greater Sydney. I was willing to travel to Mt Druitt or Granville but the courses aren't held there anymore.
If I was to buy a welder for backyard use, I'd probably just go the Boss Weld 180A from Bunnings for all the little jobs I couldn't wait to take to work to do and for anything that I thought my life or someone else's life might depend on, I'd take to my welder mate to do.
Ben.
-
3rd Jan 2021, 08:54 AM #33Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,561
That's not bad when you think about it. The average 2.5mm electrode found in shops all over the place is recommended to run at around at say 60 to 80A (will depend on type, but that is usually the range that mine fall into), so that welder will provide a duty cycle that probably exceeds actual arc time on a job (when you think about changing electrodes, chipping and positioning).
Michael
-
3rd Jan 2021, 10:14 AM #34Diamond Member
- Join Date
- Oct 2008
- Location
- N.W.Tasmania
- Posts
- 1,407
A couple of good operators.
In line with Clear Out's last comment, Bob Moffatt with Weld.com and Jody Collier with Welding tips and tricks, both on YouTube are two very good operators in my opinion. No doubt there are many others, but these two have a huge body of work out there, and any beginner and many experienced welders would find answers to problems they might have with Bob and Jody.
-
3rd Jan 2021, 05:12 PM #35Most Valued Member
- Join Date
- Nov 2007
- Location
- melbourne australia
- Posts
- 3,228
Thanks Michael for that useful feedback. Based on that I'll put one of those machines on my birthday wish-list.
Regarding TAFE welding courses- it seems like most of the posters here recommending doing a course did theirs well over 20 years ago when welders were expensive and TAFE courses were cheap. Now the reverse is true. The cheapest TAFE welding course I could find in VIC was $650 for a basic course. I can get a reasonable handyman stick welder and good helmet for less than that.Chris
-
4th Jan 2021, 06:15 PM #36
It's just a quick off the cuff response to all this (I was the original OP).
I just shelled out today for 'Bossweld 180' from Bunnings. $250.
Yes it's a toy according to you 'pros', but it's not all that bad. (I've previously suffered with a couple of ancient probably stuffed transformer welders).
Suddenly I can weld acceptably - after just about an hour. A long way from perfect- but that's mainly due to MY in-expertise.
Great little thing, and I'm sure I'll want something bigger and better one day, but what a delight to be able to get a half-decent weld so easily.
One thing I didn't really 'clock' previously, was that as well as the material thickness, electrode diameter, amperage was critical, ...what really comes into the equation is the rate of travel.
Now I have adjusted my auto visor, I can now actually SEE the work. (I was paranoid about my eyes). Previously I was burning holes in the work because I couldn't see the work properly and was moving too slow, now I can see it I'm moving faster, so nice solid continuous welds with no burned holes.
What a relief, now I can just practice, and I'll get it right.
-
4th Jan 2021, 07:23 PM #37Most Valued Member
- Join Date
- Nov 2007
- Location
- melbourne australia
- Posts
- 3,228
-
4th Jan 2021, 07:44 PM #38
No Chris, I didn't push my luck!
A test for later I think - pushing the duty cycle. I'll do a test once I'm happy with a basic weld, and report back.