Vision quality through welding mask auto-glass
I am just starting my adventure with MIG welding.
I bought "economically priced" welding helmet, which
is equipped with sensitivity, and darkening level
controls. I have tried various settings, and set it like
midway both.
While welding I either see barely anything, or after
trigger is pressed I see very bright arc but not the
piece that I am trying to weld. Why ?
- is it because of the quality of auto-glass (or lack thereof) ?
- is it because of the age (close to retirement) ?
- is it because of the light level (indoors) ?
- is there any other factor involved ?
or it is just a combination of all above, and I should
simply get used to it and develop other senses to
figure which way I should move the torch ?
-
6th Dec 2020, 08:36 AM #2Most Valued Member
- Join Date
- Jul 2010
- Location
- Melbourne
- Posts
- 9,088
Are you sure the helmet is triggering?
You don't happen to have a lot of light coming from behind your head do you?
That can light up the inside of the helmet and make life harder than it needs to be.
-
6th Dec 2020, 09:23 AM #3Member: Blue and white apron brigade
- Join Date
- Feb 2006
- Location
- Perth
- Posts
- 7,189
flat battery?
-
6th Dec 2020, 10:50 AM #4
Me too...
I used to enjoy oxy welding, something nice and 'artful' about moving that little pool of molten metal about, but the cylinder rentals became too much for the amount of usage it got, so I surrendered it.
I hate my $10 arc welder, it works fine, but it's a horrible violent process ain't it! And...
I have the same problem with the auto helmet/visor. It's working but it's either too dark to see the work, or too bright at the arc to see the work.
I'm a little paranoid about adjusting the settings. My eyes are my only valuable asset!!!
I'm thinking of buying a cheap MIG. Should I? Would MIG be easier?
-
6th Dec 2020, 12:05 PM #5Most Valued Member
- Join Date
- Jul 2010
- Location
- Melbourne
- Posts
- 9,088
I'm a little confused. "It's working but it's either too dark to see the work, or too bright at the arc to see the work." Doesn't that mean you have adjusted it?
Is it adjustable shade or just sensitivity? If its an old fixed shade for TIG or MIG welding it may well be to dark for stick. As I recall MIG requires about 2 shades darker than stick, can't remember the number for TIG but its brighter still. But I'm old and forgetful so wait until someone agrees with me
I think you will find "pretty much" all the harmful stuff is stopped by the lens regardless(light/dark on/off)
Can't help with the "easier" part, as I have never stick welded with an auto helmet.
-
6th Dec 2020, 12:55 PM #6
Thanks
It's a fully adjustable visor:
Auto switch on
Solar with LiIon (backup)
Auto darkening / switching time adjustable
Dark shade range setting
Light shade number (Sensitivity?)
Recovery delay adjustability
I'm sure this is a 'user issue'! Aged eyes will not be helping! ("But I'm old and forgetful") LOL.
I need to experiment a bit more. Just that so far, I've found it difficult to see where I'm going on the work because once it's 'struck' it's dark apart from the actual arc which is very bright, so it's hard to see the direction you need to go in.
Perhaps this isn't the right place to ask, but how much better would MIG be than my old arc welder, -should I spend a few hundred bucks?
-
6th Dec 2020, 01:12 PM #7Pink 10EE owner
- Join Date
- Aug 2008
- Location
- near Rockhampton
- Posts
- 6,218
Is it on grinding mode?
Gold, the colour of choice for the discerning person.
-
6th Dec 2020, 04:44 PM #8
Grinding?
Sorry I don't understand the question "is it on grinding mode".
We were talking about welding yes?
Are there welding masks that are made for grinding operations too?
-
6th Dec 2020, 05:59 PM #9Pink 10EE owner
- Join Date
- Aug 2008
- Location
- near Rockhampton
- Posts
- 6,218
Every modern new auto darkening welding helmet I have seen, even the cheap ones have grinding mode, when they will not go dark. So you can use them for eye protection when grinding.
In fact the ones I have recommend when finished use of them, to put them in grinding mode so as not to flatten the battery.Gold, the colour of choice for the discerning person.
-
6th Dec 2020, 06:05 PM #10Member: Blue and white apron brigade
- Join Date
- Feb 2006
- Location
- Perth
- Posts
- 7,189
I doubt it's in grinding mode - because even when the OP's welding its still too dark. If it was in grinding mode he would be "blinded by the light"!
When this happened to mine it turned out to be a flat battery.
-
6th Dec 2020, 06:44 PM #11
Junk helmet, bad eyes.
If you got cheap eyes, get cheap helmet.
Even something around the $300 mark is 10x better than the $40 ebay specials, or the $80 'home brand' units from the usual suspects.
Welding shade is a function of Amperage, give or take a shade or so for the welder's eyes and preference.
Most MIG/MAG under 180A i'm on shade 9-10.
Most TIG is at sh9.
Where the better helmets excel is ability to identify an arc accurately at low amperages. Plus the optical clarity is waaaaay better.
after using a good helmet, Cheap ares are like looking thru a window smeared with butter...
-
6th Dec 2020, 07:28 PM #12
$2.50 eyes?
Or $2.50 brain?
So it's the old story then... the answer is to spend more money? That's 'the tip' is it?
Some of us just don't have the money to spend on the 'supposed' best equipment.
And many decades on this planet have taught me that in many many many cases, the pricey stuff is no better than the cut-price stuff.
-
6th Dec 2020, 07:58 PM #13
Hi grumpy.i.m
Welcome to the forums,
You do not tell us if you wear prescription glasses .
If you do wear glasses, the focal length of those glasses can be important. Do you require glasses to read?. See if length from eye to what are welding corresponds to your personal reading focal length
Those who don't need glasses don't appreciate this as there can be problems with the bifocal line up with that spot you are trying to weld on.
A work around can be a cheap pair of glasses as often found on a display tree in the pharmacy or sometimes in the shopping centers.These glasses are marked in different strengths with sticky labels on the glasses. One tries on the various pairs and finds what suits best..
Another factor not mentioned often is that a shield if well used will likely need a fresh clear protective lense.
As well as getting smudged externally, the lense can be covered with a gas residue from the arc. If the cover lense does not respond to a clean,replace it.
The lenses used to be referred to as 1000hr lenses but none that I used ever lasted that long.
Modern large window shields seem to use a non standard dimension lense which is either costly or not readily available in the cheaper versions.
If I hang my shield uncovered, on the wall, the dust in the atmosphere will coat the lens distorting vision to slight degree.
If you are really doing a lot of welding on a really hot and humid day, the lense can fog up from your own perspiration and a creme used on safety glasses lenses could be polished on to the lense.
With that being said it could be that the shield is not performing as it should.
I suggest doing some of those simple,easy and cheap things first ( as described in posts above ) before discarding your shield.
Grahame
-
6th Dec 2020, 10:56 PM #14
grumpy.i.m
Can you see something like this?
https://www.youtube.com/watch?v=4ZDosXn8S2g.
The welder should be able to clearly see the arc, welding wire , nozzle and a small area of the joint or area to be welded. I would say the shade if adjustable on the Utube sample could be a bit lighter, though.
Have you welded with another process or is Mig your first time ?.
If your shield window is a smaller one -say roughly- 90 x 50mm -they vary, then magnifying diopter lenses are available.Don't know about the bigger sizes.
Grahame
-
7th Dec 2020, 12:05 AM #15New Member
- Join Date
- Dec 2020
- Location
- BKK
- Posts
- 8
Yes, I do.
Originally Posted by You don't happen to have a lot of light coming from behind your head do you?
That can light up the inside of the helmet and make life harder than it needs to be.
Similar Threads
-
Auto darkening mask not darkening fix
By rusel in forum WELDINGReplies: 5Last Post: 29th May 2016, 02:55 PM -
Double banger - Duragal removal and breathing mask for welding
By twebb01 in forum WELDINGReplies: 5Last Post: 21st May 2015, 09:35 PM -
$100 Welding Mask recommendations
By DSEL74 in forum WELDINGReplies: 12Last Post: 21st Sep 2014, 10:41 AM -
best welding mask?
By Goldfields in forum WELDINGReplies: 7Last Post: 23rd Aug 2010, 02:21 PM -
Welding Mask
By 19brendan81 in forum WELDINGReplies: 29Last Post: 13th Aug 2009, 07:21 PM