I want to replace the damaged tip of a vintage shovel,, normally I just reshape them with a grinder but why not weld a piece of similar steel on and reshape that ..the shovel is 1.7 mm thick and I have a few donor shovels to cut up.
Has anyone tried it before ?
ken
-
2nd Dec 2020, 12:41 PM #2
I have not tried it but am aware of the following.
Believe or not the metallurgy of a shovel is getting up there with the higher carbon steel tools.
Mig if you have one using LW1 wire should put you close. Alternate is a stick inverter using LH electrodes and quick short run then moving somewhere else where metal is cold .Rinse and repeat.
If using stick , weld with hotter amps than normal and travel real fast.
In other words don't concentrate all that heat in the one spot. Weld a short bit and move away.
Grahame
-
2nd Dec 2020, 01:46 PM #3China
- Join Date
- Dec 2005
- Location
- South Australia
- Posts
- 1,658
You could Oxy Acetylene same method as they used to use on car bodies ( some still do) weld 20-30 mm hammer flat move to other side same thing the back to the first side and so on until done
Similar Threads
-
Tig welding
By eskimo in forum WELDINGReplies: 43Last Post: 16th May 2020, 12:00 PM -
Welding gal
By Groggy in forum WELDINGReplies: 6Last Post: 10th May 2009, 11:00 PM -
Gas Axe Welding Set
By watson in forum METALWORK GENERALReplies: 14Last Post: 30th May 2008, 05:52 PM -
new to welding.
By Bluegum in forum WELDINGReplies: 8Last Post: 24th Oct 2006, 09:22 PM -
welding tip
By mako in forum WELDINGReplies: 4Last Post: 7th Jul 2006, 04:59 PM