    Default Corner Clamping Tapered Parts?

    Hi there!
    I hope this is the correct area to ask, but I'm about to do a bunch of brazing on 0.125 aluminum foot shell parts (about two dozen) for a full size Star Wars R2D2 build.
    Problem I'm having is that R2D2's feet / these parts are pyramid shaped and requires a weird corner clamp angle I'm not sure how to achieve.

    For instances, the very first parts you put together are corner welds, but tapered out:


    Normally I would just square my parts up by eye and let it rip, but because there are so many parts here that need replica precision, I want to get things truly squared up and not just by eye.

    How do you normally clamp a 90deg corner that tapers?

    Thank you in advanced!

  2. #2
    Join Date
    May 2011
    Location
    Murray Bridge S Aust.
    Age
    68
    Posts
    4,719

    Default

    Hi Devin, and WELCOME to a TOP FORUM.
    I'd make 2 corner blocks out of 2" X 1/4" flat bar, at the correct angle, one for each side that can be clamped to the Aluminum to hold in the correct position.
    Having the flats sitting on a sheet of steel will allow a magnet to hold it all in place.
    HTH
    Kryn
    To grow old is mandatory, growing up is optional.

  3. #3
    Join Date
    May 2013
    Location
    Rockhampton, QLD
    Age
    65
    Posts
    330

    Default

    Welcome to the forum Devin.

    Ross

Similar Threads

  1. Tapered pipe threads - are the sockets usually tapered too?
    By OxxAndBert in forum METALWORK GENERAL
    Replies: 8
    Last Post: 1st Sep 2020, 04:39 PM
  2. Making a Corner Notcher
    By KBs PensNmore in forum METALWORK GENERAL
    Replies: 0
    Last Post: 19th Feb 2019, 09:08 PM
  3. Help with corner to corner join
    By Tegmark in forum WELDING
    Replies: 10
    Last Post: 25th Jun 2015, 06:27 PM
  4. Internal corner technique
    By Legion in forum WELDING
    Replies: 2
    Last Post: 21st Oct 2013, 09:23 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •