    Default Any ideas where to get plastic welding rods in Perth

    The front hatch on my caravan has a plastic lid which are renowned for cracking. At about $800 to replace Im thinking plastic welding up the cracks might be a way to get a bit more life out of it.
    I have a Leister hot air plastic welder that I used to use for heatshrink so just need the rods.

  2. #2
    BobL is offline Member: Blue and white apron brigade
    Join Date
    Feb 2006
    Location
    Perth
    Posts
    7,189

    Default

    What sort of plastic is it?
    You absolutely need to know because you can't just use any old plastic as welding rods

    You can make rods yourself by cutting up 3 - 4 mm wide strips of the same plastic. The rods don't have to be round, they can be square or rectangular

    If it's cracking it sounds like it might be UV degraded in which case welding it could be a waste of time.

    Instead of welding what about making up a complete cover from scratch?

    Some photos would be useful.

  3. #3
    Join Date
    Apr 2018
    Location
    Perth
    Posts
    168

    Default

    Am looking at other options besides welding. Could bend up a new lid but now thinking , Ive got heaps of the ramset epoxy anchor tubes so thinking might tape off the cracks on outside , rough up the inside and then apply the epoxy. If it sticks then respray the cover.

  4. #4
    BobL is offline Member: Blue and white apron brigade
    Join Date
    Feb 2006
    Location
    Perth
    Posts
    7,189

    Default

    Quote Originally Posted by Sparksy View Post
    Am looking at other options besides welding. Could bend up a new lid but now thinking , Ive got heaps of the ramset epoxy anchor tubes so thinking might tape off the cracks on outside , rough up the inside and then apply the epoxy. If it sticks then respray the cover.
    Sounds like a plan but if it's Polyethylene or polypropylene even if it's roughed up the epoxy won't hold for long. Looks up plastic burn tests on the web - then cut off a thin sliver and see what it is.

  5. #5
    Join Date
    Dec 2005
    Location
    South Australia
    Posts
    1,658

    Default

    Bunnings

Similar Threads

  1. Plastic welding?
    By jabell in forum WELDING
    Replies: 12
    Last Post: 20th Jun 2018, 08:17 AM
  2. Large plastic chopping board at ALDI - good plastic stock
    By pippin88 in forum METALWORK GENERAL
    Replies: 1
    Last Post: 3rd Jul 2017, 10:24 PM
  3. Plastic Welding
    By foaley77 in forum WELDING
    Replies: 9
    Last Post: 26th Jul 2010, 01:06 AM
  4. El cheapo welding rods
    By Charleville in forum WELDING
    Replies: 29
    Last Post: 29th Jul 2008, 04:16 PM
  5. Welding Rods
    By lnt9000 in forum WELDING
    Replies: 1
    Last Post: 20th Feb 2008, 07:30 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •