Token tools Alupulse 210 Pro - who's got one?
Hi all,
My original (circa 2007) Token Tools 200a AC/DC TIG is slowly on its way out, so I'm looking to upgrade.
https://weldingstore.tokentools.com....welder-210pro/
The different AC waveforms on top of standard square wave, and a AC + DC hybrid mode is very appealing, as I do a lot of thin aluminium.
Programmable memory slots are a big plus, but not sure how many there are.
I did find that the waveform selections for AC and duty cycle are the same as the Miller Dynasty 210 DX.
Who has one?
What don't you like about them?
What is great about them?
Worth the $2700 with the foot control?
Cheers!
-
2nd Aug 2020, 05:33 PM #2Member: Blue and white apron brigade
- Join Date
- Feb 2006
- Location
- Perth
- Posts
- 7,189
Yep I have one. I don't use it a lot but it has never disappointed.
The only problem I've had was an overly tight fitting bayonet on one of the cables which I was able to fix with two swipes of a file.
I love the memories - saves a lot on my own.
Mine has 8 - I think.
With an Ar reg, std torch and pedal (still haven't used it) mine cost $1800 5 years ago.
Yes I would buy another.
-
4th Aug 2020, 01:10 AM #3Novice
- Join Date
- Sep 2016
- Location
- mandurah wa
- Age
- 75
- Posts
- 10
I've got the 215 Multi process model , which has the combined plasma cutter, I had a minor issue with the hf start but a quick call to Pete at Token and he ran through it with me to find I had a slightly out of adjustment points.
No issues since but have only used for aluminium so far. IMO a good machine with great back up if needed.
-
4th Aug 2020, 10:43 AM #4Novice
- Join Date
- Apr 2013
- Location
- Mornington Peninsular
- Posts
- 23
I also have the 215 multi process - I already had a plasma cutter, but it wasn’t much more and now I have two!
I also got the foot control and the mini torch. This is great for light work - it’s almost like a pencil with a very light cable.
No problems in 5 years.
Sent from my iPad using Tapatalk
-
4th Aug 2020, 11:01 AM #5Most Valued Member
- Join Date
- Jul 2006
- Location
- Athelstone, SA 5076
- Posts
- 4,258
I have one but am still learning how to use it...or in other words I still cant do nice TIG welds...plasma works great
Similar Threads
-
Internal Pics of Token tools Metalmaster AC DC 210 Tig
By bj48 in forum WELDINGReplies: 6Last Post: 1st Oct 2018, 11:38 PM -
Token tools welder
By eskimo in forum WELDINGReplies: 23Last Post: 18th Aug 2017, 09:01 PM -
Token Tools MMA selection - need help!
By twebb01 in forum WELDINGReplies: 6Last Post: 18th May 2015, 07:00 PM -
Token tools cyber sale
By mac_man_luke in forum WELDINGReplies: 0Last Post: 1st Dec 2014, 08:25 PM -
Token Tools Alupulse 200 AC/DC Tig Welder
By steran50 in forum WELDINGReplies: 9Last Post: 14th Mar 2011, 12:24 AM