    Default Best Way To Weld Table Frame (Square)

    Hi all just wondering what’s the best way to weld a table frame and keeping it all square.Looked a lot on youtube but can’t find a solid solution.
    Thanks in advance Best Way To Weld Table Frame (Square)


    Sent from my iPhone using Tapatalk

  2. #2
    Join Date
    Dec 2005
    Location
    South Australia
    Posts
    1,657

    Default

    Welding magnets, corner clamps, clamping to a table, tack everything in place the do the full welds.

  3. #3
    Join Date
    Jan 2016
    Location
    Wodonga Vic
    Age
    38
    Posts
    633

    Default

    Measure opposing corners after tack welding and make sure they're equal, if they aren't equal they aren't square

  4. #4
    Join Date
    Aug 2006
    Location
    Melbourne
    Posts
    1,106

    Default

    Then there is welding sequence as well, weld corners first etc. Spread heat around. Keep gaps to a minimum.

  5. #5
    Join Date
    Dec 2018
    Location
    NSW
    Posts
    586

    Default

    Also worth mentioning that you can be square in the XY plane (ie both corner to corner measurements are equal), but warped in the Z.
    An easy trick is to run two string lines across opposing corners, and check that string touches where they meet in the middle- if they do it's flat. Working on a flat surface really helps, but not everyone has that luxury.
    Do this measurement after tacking, and keep heat control under check while doing the final weld out.

  6. #6
    Join Date
    Apr 2019
    Location
    Adelaide
    Posts
    596

    Default

    Have a look at the YouTube videos from Fireball Tool. Jason is pretty talented;

    How To Stop Parts Warping - https://www.youtube.com/watch?v=lL98oE2NaQg

    Fireball Tool Squares - https://www.youtube.com/watch?v=d-DwdsegIks


    I bought a couple of his squares and they look spot on.

  7. #7
    Join Date
    May 2011
    Location
    Murray Bridge S Aust.
    Age
    71
    Posts
    5,959

    Default

    We use turnbuckles to help hold things square, also putting diagonal braces helps hold things where they should be.
    As others have mentioned, stagger the welding sequence, and don't put too much heat in the one corner.
    To grow old is mandatory, growing up is optional.

  8. #8
    Join Date
    Sep 2019
    Location
    Melbourne
    Posts
    23

    Default

    Quote Originally Posted by Mk1_Oz View Post
    Have a look at the YouTube videos from Fireball Tool. Jason is pretty talented;

    How To Stop Parts Warping - https://www.youtube.com/watch?v=lL98oE2NaQg

    Fireball Tool Squares - https://www.youtube.com/watch?v=d-DwdsegIks


    I bought a couple of his squares and they look spot on.
    Thanks all for help.Mk1 that’s probably the best video available on YouTube.
    The Fireball Tool looks great but they not cheap.
    Thanks heaps all


    Sent from my iPhone using Tapatalk

  9. #9
    Join Date
    Jul 2006
    Location
    Athelstone, SA 5076
    Posts
    4,258

    Default

    Quote Originally Posted by Mk1_Oz View Post
    Have a look at the YouTube videos from Fireball Tool. Jason is pretty talented;

    How To Stop Parts Warping - https://www.youtube.com/watch?v=lL98oE2NaQg

    Fireball Tool Squares - https://www.youtube.com/watch?v=d-DwdsegIks


    I bought a couple of his squares and they look spot on.
    why didnt you send the link a few years ago

  10. #10
    Join Date
    Apr 2008
    Location
    Southern Riverina
    Posts
    24

    Default

    If you haven't got a flat surface to start with, you can fake one with a couple of straight bits of steel (or even timber). Use a spirit level and shims etc to get them level first, then work off them.

Similar Threads

  1. Box tubing clamp for holding table leg to table frame
    By 19brendan81 in forum METALWORK GENERAL
    Replies: 4
    Last Post: 11th Jan 2017, 12:05 PM
  2. Replies: 51
    Last Post: 30th May 2016, 08:24 AM
  3. Replies: 34
    Last Post: 17th May 2015, 10:39 PM
  4. Square tubing that's not square
    By Corgan in forum METALWORK GENERAL
    Replies: 18
    Last Post: 1st Nov 2011, 09:31 AM
  5. Table square block for miller
    By Grahame Collins in forum METALWORK GENERAL
    Replies: 14
    Last Post: 13th Mar 2011, 08:26 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •