ha,ha, ok,but we are going to have to agree to disagree. i,ve had a few bourbons , so i,ll be direct.
i,ve tigged up stacks of pipe , but not much stick, but what you say "flies in the face" of traditional stick welding training. i don,t believe for a minute that the fill is done with 6010, and any good welder is happy to run a low hydrogen rod. but it doesn,t matter what i say, its the welding procedure that is done by welding engineers is that what is strictly followed. these are critical welds. you can quote all numbers but the welding engineer is the man, and we must do what is required.
i think i said i worked with structural steel, buildings, bridges, tanks etc.. structural steel is all migged up, and thats low hydrogen. only site mods and tricky spots require a stick welder. , structural steel we mainly worked with is 350 grade.
-
4th Jul 2020, 09:19 PM #17Pink 10EE owner
- Join Date
- Aug 2008
- Location
- near Rockhampton
- Posts
- 6,218
-
5th Jul 2020, 03:59 PM #18
To be fair this is the same for any electrode stored out of its original packaging out in the wild. Proper electrode care should be part of any meaningful weld procedure.
The good low hydrogen rods come in a sealed ring-pull can or a vac sealed pouch.
16TCs are in a very mediocre plastic wrap which is held together with hopes and dreams... not the best for resisting moisture ingress IMO.
Similar Threads
-
Equivilent RHS/SHS in U Beam?
By gazza2009au in forum TRAILERS & OTHER FABRICATED STUFFReplies: 33Last Post: 17th Jul 2018, 01:39 PM -
Beam deflection
By Gestalt in forum METALWORK GENERALReplies: 32Last Post: 25th Nov 2017, 07:11 PM -
Building a Aluminium I Beam Trailer
By gazza2009au in forum TRAILERS & OTHER FABRICATED STUFFReplies: 58Last Post: 30th Mar 2015, 11:45 PM -
Cornish beam engine
By neksmerj in forum METALWORK GENERALReplies: 5Last Post: 22nd Aug 2013, 01:05 PM -
Electrode positive or Electrode negative
By .RC. in forum WELDINGReplies: 8Last Post: 26th Apr 2009, 12:39 AM