joining brass
I have two brass or bronze hinges. I want to join them, edge of leaf to edge of leaf. I have a MAP/Air torch. I assume I would need to braze them. What type of brazing rod would I use? Is this the right approach? Will I be able to machine the join afterwards?
Many thanks in advance
Paul
-
15th Jun 2020, 11:29 PM #2Senior Member
- Join Date
- Oct 2015
- Location
- melbourne
- Posts
- 473
How thick are the leaves?
Yes, braze, or perhaps silver solder, would work, but if they aren't thick enough the joint will not be strong. That may not be an issue, depending on the application.
If the join is at right angles you may be able to strengthen with a small fillet?
-
16th Jun 2020, 08:30 PM #3
Hi betchernOt,
Welcome to the MetalWork Forums,
The following is a guide to getting started on the forum.
If you click on the down arrow in the FORUM box -Top LH corner
A pull down menu appears by clicking Forum Home. Click Forum Home and it takes you to a scroll -able page.
The Terms of Use please read them are right on top and the rest as you scroll down are help areas and sub forums . Some of the sub forums have stickies on top to guide the user.
We are privileged to have a group of big hearted and helpful folk here.
Welcome to the group.
Grahame
-
16th Jun 2020, 08:57 PM #4Most Valued Member
- Join Date
- Jul 2006
- Location
- Athelstone, SA 5076
- Posts
- 4,258
you can also use 15% -45% silver brazing rods. Use with flux.
Map gas will do it okay.
Similar Threads
-
what rods for thin brass to brass ??
By Mathuranatha in forum WELDINGReplies: 7Last Post: 23rd Nov 2020, 08:17 PM -
Joining two 8mm shafts. Best way?
By jhovel in forum METALWORK GENERALReplies: 18Last Post: 7th Feb 2016, 12:28 AM -
VICTORIA Brass Flat Bar Assorted Sizes & 1/4" SWB Threaded Rod & 260 Carbide Brass Sheet
By thumbsucker in forum METALWORK - Machinery, Equipment, MARKETReplies: 7Last Post: 18th Mar 2013, 03:36 PM -
Joining nails - need help.
By JustWondering in forum METALWORK GENERALReplies: 2Last Post: 16th May 2007, 06:08 PM