4th Jan 2020, 05:36 PM #1Golden Member
- Join Date
- Nov 2005
- Location
- adelaide
- Posts
- 597
transmig 195 rural pack
been offered one of these for an affordable price not this one its a bit tackier on the outside
anything to look out for want to have a go at
welding ally i have gas from useless chinese buy
pic for ident
-
4th Jan 2020, 11:28 PM #2Most Valued Member
- Join Date
- May 2011
- Location
- Murray Bridge S Aust.
- Age
- 71
- Posts
- 5,959
I'm pretty sure that they are almost bulletproof.
I suggest that you contact WESS Welding Equipment Sales and Service at Cormack Rd Wingfield, for more details re spares etc if required, they've been around a looooong time, about 30+ years, so if there were any problems with them, they'd know.
HTH
KrynTo grow old is mandatory, growing up is optional.
-
5th Jan 2020, 03:56 PM #3Golden Member
- Join Date
- Nov 2005
- Location
- adelaide
- Posts
- 597
Thanks Kryn i have put off inspection till i contact WESS as you advised
cheers john
-
6th Jan 2020, 03:28 PM #4Senior Member
- Join Date
- Apr 2008
- Location
- Perth
- Posts
- 269
CIG Rural Pak
Fantastic welder, bought one new in the 1980’s from CIG in Karratha, learned to weld aluminium with it.
The day I sold it to a boilermaker in the mining town I lived in was a sad one, as I was leaving that job for another I could not fit it my trailer.
Found that welder to be one if the best Mig’s I have owned.
DD
-
6th Jan 2020, 07:28 PM #5Golden Member
- Join Date
- Nov 2005
- Location
- adelaide
- Posts
- 597
thanks DD well i got it home took all then covers off ( it not pretty on the outside) blew out 1/2 a kilo of dust didnt have a regulator but i had a cig one off a cheap chinese one i bought a new shroud and some gas a new roll of .8 mm wire and promptly welded the wire to the tip
back to the welding shop for more tips and upped the wire feed rate and voila it worked but a bit of fine tuning to go
thanks every one for your support
john
Similar Threads
-
Rural Pak 195
By ptrott in forum WELDINGReplies: 4Last Post: 20th Dec 2017, 05:55 PM -
Cowra Rail, War and Rural Museum clearing sale
By Canoath in forum ANNOUNCEMENTSReplies: 4Last Post: 12th May 2016, 01:30 PM -
Transmig 195 Rural Pack 2
By Brian.Y in forum WELDINGReplies: 9Last Post: 18th Jul 2014, 11:21 PM -
Transmig 195 Rural pack 2 - consumables question
By ntboozer in forum WELDINGReplies: 5Last Post: 17th Feb 2014, 05:51 PM