    Smile spot welding 18 gauge

    My jeep project is coming along the engine is down at the machine shop ATM . I'll be needing to spot weld 1.2mm panels and 1.6 to 1.2 mm stuff together for the tub repairs. Will a 240 V single phase spot welder be OK for this type of work ? I'm looking for a used machine with suitable amperage .

  2. #2
    Join Date
    Oct 2011
    Location
    Norwood-ish, Adelaide
    Age
    59
    Posts
    6,542

    Default

    It should do it. The key thing will be to make sure that your point tips are small enough so you get decent current density. Check using peel tests.

    Michael

  3. #3
    Join Date
    May 2011
    Location
    Murray Bridge S Aust.
    Age
    71
    Posts
    5,945

    Default

    Mike, do you have a MIG welder? If you have, then that can be utilised as one. If you set your nozzle up so that it has 4 "castles", as below, so that they will allow the gas to vent, then push down and apply the trigger. Get some scrap pieces to practice and get your settings and time right. Some of the MIG welders have a setting for spot welding.
    MIG Spot welding Nozzle.jpg
    HTH.
    Kryn
    To grow old is mandatory, growing up is optional.

  4. #4
    Join Date
    Jul 2008
    Location
    near Warragul, Victoria
    Posts
    3,718

    Default ok

    Thanks Kryn

    This doesn' t sound promising
    AutoSpeed - Spot welders for the home workshop, Part 1

  5. #5
    Join Date
    Jul 2008
    Location
    near Warragul, Victoria
    Posts
    3,718

  6. #6
    Join Date
    Oct 2011
    Location
    Norwood-ish, Adelaide
    Age
    59
    Posts
    6,542

    Default

    Not quite

    Michael

  7. #7
    Join Date
    Oct 2007
    Location
    Alexandra Vic
    Age
    69
    Posts
    654

    Default

    Quote Originally Posted by morrisman View Post
    A standard method for pulling out small dents and depressions these days is to weld threaded studs into the depression, then screw on a slide hammer to manipulate the metal and pull it back into shape. The studs are then broken off and any residual weld is ground off, aiming to leave a clear surface slightly below the desired finished surface. The slight depression is then filled with a minimal amount of filler and contoured to the final shape.

    The gizmo you linked is the welder for placing the studs for the above technique. Functionally it is a spot welder, but the current density and pressure are not adequate to form permanent bonds, they produce a temporary bond intended to broken by twisting the stud with a pair of pliers or vice grips.

    For spot welding sheet metal, you are looking to something like this . The tips compress the panels together with a reasonable amount of pressure then a short high current pulse of electricity passes through the tips and compressed metal fusing it together permanently.

    Another alternative is to drill/punch holes in one panel, align and clamp the panel, then puddle weld through the holes to the other panel, slightly overfilling the hole and then grinding back to flush.

    Hope this helps.
    I used to be an engineer, I'm not an engineer any more, but on the really good days I can remember when I was.

  8. #8
    Join Date
    Dec 2005
    Location
    South Australia
    Posts
    1,656

    Default

    While searching for something else entirely I came across this you may want to investigate

    https://www.ebay.com.au/itm/Alpha-Sp...ad76%7Ciid%3A2

Similar Threads

  1. spot welding in Brisbane
    By kenny_10 in forum WELDING
    Replies: 3
    Last Post: 2nd Apr 2019, 12:50 PM
  2. NZ Swap on the Spot Gas
    By KBs PensNmore in forum WELDING
    Replies: 2
    Last Post: 21st Feb 2015, 11:58 AM
  3. spot welding aluminium
    By morrisman in forum WELDING
    Replies: 2
    Last Post: 31st Mar 2013, 11:03 PM
  4. Spot welding electrodes
    By Michael G in forum METALWORK GENERAL
    Replies: 11
    Last Post: 1st Feb 2012, 06:20 PM
  5. Spot Welder
    By Keith_W in forum WELDING
    Replies: 4
    Last Post: 5th Apr 2009, 09:16 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •