Needs Pictures: 0
Picture(s) thanks: 0
Results 1 to 15 of 25
-
17th Dec 2019, 08:33 PM #1Most Valued Member
- Join Date
- Jul 2010
- Location
- Melbourne
- Posts
- 9,088
Its time for a TIG, but what options?
Evening
Having had almost nothing to do with TIG welding for around 30 years I've decided its time for me to buy one. I know the basics though all my welding was on transformer based machines, only one having amperage control on the hand piece(though I barely remember using it).
I want high Freq
I want to weld Alum
Token Tools gets a thumbs up from a few around here.
Plasma is a bonus
So this looks the part
https://weldingstore.tokentools.com....elite-digital/
My questions really start with the options.
Never used a flex head, for the extra $10 is it a no brainer? or is there a trap I don't know about with them?
As most of the welding I see myself doing will be on the light side I was thinking about adding 9 series torch.
I assume foot control is the way to go???
Reg, Gas and some rods and I am good to go, or have I forgotten something?
-
17th Dec 2019, 09:53 PM #2Golden Member
- Join Date
- Mar 2009
- Location
- Melbourne
- Age
- 54
- Posts
- 825
Add a pair of tig gloves to the list and if you have an auto helmet make sure you can adjust the shade beyond 9 as tig is brighter than stick or mig, particularly on ally.
I'd recommend using a gas lense over a standard nozzle/cup, not essential but allows you to stick the electrode out further which can make life easier getting into tight spots.
Get an assortment of electrode types, ceriated for steel and zirconiated for ally. Thoriated scare my testicles so I give them a miss and I've not had a lot of luck with rare earths but that may well be something I'm doing wrong.
Cheers,
Greg.
-
17th Dec 2019, 10:46 PM #3
Yep the little 9 torch is the go for probably 90% of steel but could be on the lacking for Al as you need much higher amps, personally I went for a 20 series(same as a 9) with a matching water cooler I can keep that sucker pegged until the tig machine calls it quits!(hasn't happened yet...)
Flex head would be handy for tight spots but a button back cap and a small gas lense is tiny enough on a 9 series, I would suggest steering clear of a bulky euro handle and go for a yanky straight sleeve with a micro switch zip tied to it for when the foot pedal is not practical.
I use 2% lathinated electrodes for everything 1.6mm for most welding and 3.2mm for 120 amps plus(like on Al), I personally think matching rod thickness to material is more important than electrode dia unless your intending working to aerospace specs.
So grab an assortment of rod dia for steel, buy a small spool of mig wire for the thin stuff and some 1kg packs of 1.6, 2.4 and 3.2 ER70S2 or S6, the thickness has a big effect on puddle cooling.....................................................................
-
17th Dec 2019, 10:49 PM #4Member: Blue and white apron brigade
- Join Date
- Feb 2006
- Location
- Perth
- Posts
- 7,189
Second a decent pair of TIG gloves,
FWIW I bought the pedal and have used it once in 3 years.
RE Thoriated Tungsten Electrodes.
Different if it was TIG shop with lots of TIG welders operating all day and year with Thoriated electrodes, but for DIY use I'd be more concerned about other things like, Chromium oxide generated when welding SS, and other fumes.
All welding, even TIG generates fumes and particulates - maybe consider getting yourself an exhaust fan?
Thorium is an alpha emitter which are stopped by a few cm of air or the outermost dead layers of your skin skin and even if it gets inside of you it has very low activity (half life of 14.05 billion years, about the age of the Universe).
The internal inhalation/ingestion risks come from two sources, dust from electrode tip grinding and fumes from eroding of the tip when welding. This has been studied in some detail and it was found that professional TIG welders (welding for 2000 hours a year) are exposed to between 1 and 21% of the maximum permissible radiation dose for industrial workers. Of course this does not take into account that some welders could accidentally overdose by eg working in significantly more confined spaces. For this reason they are being phased out in some countries.
Of course if you have a purchasing choice between by thoriated on non-thoriated electrodes then you might as well buy non-thoriated but if for example you come across thoriated electrodes for free then using them in a DIY situation should present a low risk relative to other things that go on in a DIY welding situation.
-
18th Dec 2019, 08:00 AM #5Most Valued Member
- Join Date
- Nov 2017
- Location
- Geelong, Australia
- Age
- 57
- Posts
- 2,666
Re plasma being a bonus, my experience is that it's a PITA to change out the torch from TIG to plasma and swap from gas to compressed air for cutting. My TIG has plasma function but I've only used it twice.
I've now got a cheap Aldi plasma. Plug in and cut - done!
If you're planning any stainless work get a small stainless wire brush for brushing off the oxides as the job cools. Dedicate it to stainless work and label it so it doesn't get contaminated with other crap.
I've got one for stainless and one for aluminium.
Steve
-
18th Dec 2019, 09:24 AM #6Diamond Member
- Join Date
- Jun 2010
- Location
- Canberra
- Posts
- 1,322
My accumulated wisdom - you only need one type of tungsten: 2% lanthinated, you only need one size: 3.2mm (since they're sharpened to a point).
-
18th Dec 2019, 12:09 PM #7Senior Member
- Join Date
- Sep 2019
- Location
- Newcastle, AU
- Posts
- 238
I have arthritis in the hands and find the flex head to be massively helpful - sometimes my hands/wrists don't want to bend a certain way and being able to contort the head to work around that is very helpful.
-
18th Dec 2019, 04:35 PM #8Senior Member
- Join Date
- Nov 2019
- Location
- Brisbane
- Age
- 69
- Posts
- 452
Tig welding
Hello JC.
I have a few customers with the same problem and I suggest fitting a cheap lever operated switch that attaches with cable ties. You can rotate the switch around the handle to get comfortable. I would suggest smaller tungstens for lower current as the arc carona will be more stable and when you grind the tip it is a cheaper item you shorten. A short back cap gets better access and is better that cheap flex head torches. They can't take the pace if you run them hot.
Regards
BC
-
19th Dec 2019, 10:50 PM #9Most Valued Member
- Join Date
- Jul 2010
- Location
- Melbourne
- Posts
- 9,088
Hmmm perhaps I should have said "Once upon a time I knew the basics". I'm sure there was only two types of tungsten back then lol
Thanks all, Lots to think about and chase up.(I started a longer reply but its doing my head in)
Tig gloves are just like riggers gloves with a cuff?
I've heard of gas lense but never used. I'll add kits for whatever torches I end up with.
Are tig fingers as handy as youtube make them out? Still for $9 how bad could they be?
I dont foresee doing large amounts of high amp work(certainly not in a hurry)
I do have some TIG torches around here some place I will have to dig them out. $10 says they have the wrong plug.
I see that you are saying about two machines but I'm more pushed for space than I used to be. I wonder if it would be possible to rig up some valves/quick connects to make change over faster?
I knew you needed to keep your SS stuff separate..... I just forgot is all
-
19th Dec 2019, 11:43 PM #10Member: Blue and white apron brigade
- Join Date
- Feb 2006
- Location
- Perth
- Posts
- 7,189
-
20th Dec 2019, 07:12 AM #11Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,559
Not quite. Tig gloves are relatively thin, on the basis that thick gloves would hamper manipulating the filler wire. It may be that you need to buy a few different pairs and see which ones suit.
They are certainly not essential. Yes, they make things easier in some cases but in others make little difference. Again, will depend on what you plan to do.
I have a couple and have not used them in the 12 months I've had them. I find that in most cases I don't rest my hand on the job being welded, either because I can't or it's too hot. Certainly get one to try out if you wish, but like the gas lens, it will depend on what you are doing.
The key thing will be air in your gas line, so every time you change you will need to make sure you purge the line properly - otherwise you will burn up tungstens.
HTH Michael
-
20th Dec 2019, 09:45 PM #12Most Valued Member
- Join Date
- Jul 2010
- Location
- Melbourne
- Posts
- 9,088
Am I right in assuming you don't have amp control on the torch?
We used to tig with the same gloves we miged with, so now I know why I was never that great with filler. I did enjoy fusion end welding with no filler.
Don't have anything super hard planned but you never know. I cant see myself trying to make a "stack of dimes" anytime soon.
Failing that I wonder how much another gas solenoid would cost? Starting to sound like a project I will never get around to. If I find I use the plasma enough I might just buy a cheapy. Though with a pretty quick look I couldn't find a cheap one with pilot arch, if that is indeed as handy as they say. No idea, only ever used plasma on a cutting table with new sheet. Then there is the whole "finding some where to put it" thing.
These are the torches I have. Of course they use a different plug. Also two torch kits that strangely don't actually fit those torches(except one stray collet). In fact they look like they might fit the new torches. Still if I can get/make an adapter I have the high amp rigid head side of things covered. So I might go with flex heads on the new ones. WOW I am starting to make it sound like I will be welding 12 hours a day!
Wasn't in a hurry to buy, was going to wait until the Christmas rush was over, now I dont have a choice, they are closed until 13th Jan
I guess it will give me time to loose enough weight to fit into my welding jacket again lol
-
21st Dec 2019, 07:27 AM #13Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,559
I once had a professional welder tell me that you only 'need' some form of real time amperage control for Al, simply because all other metals don't suck heat out so quickly. For us happy amateurs, I would suggest that something, whether a pedal or thumb control, is necessary while we develop the ability to do without.
Pilot arc is another of those nice to have things. I have a plasma cutter with a drag tip and it works fine. A pilot arc will just mean that you don't have to have direct tip to metal contact to start. Does that matter? I imagine not unless you are doing lots and lots of cutting. I find my cutter handy but realistically probably use it far less than 10hrs p.a., so for me pilot arc is not something I would go out and chase. (I got this cutter secondhand for a job I did some years back - I would not have even bought it if not for that.)
Michael
-
25th Nov 2020, 10:19 PM #14Most Valued Member
- Join Date
- Jul 2010
- Location
- Melbourne
- Posts
- 9,088
Can't say I don't move fast
Having ummed and arrred for the best part of a year and talked a guys ear off, I decided with many of these things some people are going to like them, some aren't and there is no way to know in advance which I would use and which I wouldn't..........So my solution was just to ticked every box. Ordered Saturday afternoon (posted Monday), arrived today.
Thanks to all for your input
Now to find out after 30 years I cant TIG weld anymore.
-
26th Nov 2020, 01:47 AM #15
What did you end up with Stu?
I bought one recently too: an AIG 200T
AC-DC, pilot arc and very happy with it so far.
They were very good to deal with and have allowed me to modify the connector and internal connection to fit a pedal to it without voiding the warranty.
Can't get better than that....
Cheers
JoeCheers, Joe
retired - less energy, more time to contemplate projects and more shed time....
Similar Threads
-
Building a shed - long time viewer, first time poster!
By bj_dove in forum WELDINGReplies: 44Last Post: 24th Aug 2014, 07:51 PM -
Trailer Options
By zuffen in forum TRAILERS & OTHER FABRICATED STUFFReplies: 8Last Post: 13th Feb 2012, 08:38 AM -
Pan Brake Options?
By browny in forum METALWORK GENERALReplies: 2Last Post: 28th Apr 2007, 05:50 PM