Needs Pictures: 0
Results 1 to 15 of 23
-
12th Aug 2019, 05:55 PM #1Most Valued Member
- Join Date
- Aug 2009
- Location
- Sydney, NSW, Australia
- Posts
- 1,844
Prep advice? Going to tig this hole
Going to weld up this hole first option was mig but i dont have a teflon liner so going to fire up the tig and have a go, i have a piece if 100x50x3 brass backing shop didnt have copper
Any advice on cleaning? I am know to be not so clean and get impurities in the weld
Finger is for reference, was quoted $200 to repair, $300 for a new starter but i need the practice
-
12th Aug 2019, 06:34 PM #2Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,562
Brass is no good - the zinc will come out and play havoc with the weld. It needs to be copper.
Michael
-
12th Aug 2019, 06:51 PM #3Most Valued Member
- Join Date
- Aug 2009
- Location
- Sydney, NSW, Australia
- Posts
- 1,844
Thanks Michael any idea what i can use for backing? The steel shop is 30mins each way away
-
12th Aug 2019, 07:10 PM #4Most Valued Member
- Join Date
- Nov 2017
- Location
- Geelong, Australia
- Age
- 57
- Posts
- 2,673
If you've got a bit of copper water pipe you could try flattening that.
Steve
-
12th Aug 2019, 07:55 PM #5Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,562
Rather than try to fill the whole lot, my preferred method would be to neaten up the hole and make up a patch to match. The whole thing will need to machined anyway before it's able to be used, so build up can be tolerated.
Michael
-
12th Aug 2019, 08:50 PM #6Most Valued Member
- Join Date
- Aug 2009
- Location
- Sydney, NSW, Australia
- Posts
- 1,844
Thanks for that idea Steve bunnings is just around the corner
Michael thats an idea it will save a lot of gas and i have some 4mm sheet in the shed will hitting the aluminium with a steel hammer effect how it welds?
-
12th Aug 2019, 09:22 PM #7Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,562
Shouldn't do (unless you embed bits of steel in the Al when you hit it - unlikely unless the hammer shatters )
Michael
-
12th Aug 2019, 10:59 PM #8Most Valued Member
- Join Date
- Sep 2010
- Location
- Lebrina
- Posts
- 1,915
Definitely better to make a section and then weld it in as you will get substantial shrinkage if you just fully weld it which will potentially distort far more than just the repaired area. Being a casting, it may well weld like crap, so be prepared for the odd rework. All things are possible with forethought, skill and patience. IE, think about the job, prep it well (cleanliness) and if it starts going pear shaped, then stop and reassess.
Steel or stainless will act as a backing for Aluminium. I don't personally like copper all that much for Aluminium as it tends to suck the heat away. Pay attention to letting the piece cool evenly so as to avoid cracking.
-
13th Aug 2019, 01:52 PM #9Most Valued Member
- Join Date
- Aug 2009
- Location
- Sydney, NSW, Australia
- Posts
- 1,844
Thanks for the help to those who have offered advice i made the blank bit today to fill in the hole my fitment is not 100 percent perfect there are tiny gaps i hope i can bridge these gaps without blowing a hole right thru it my machine is pre set amps so not foot peddle to vary the amps
-
13th Aug 2019, 06:54 PM #10Most Valued Member
- Join Date
- Nov 2017
- Location
- Geelong, Australia
- Age
- 57
- Posts
- 2,673
Does your welder have a downslope setting?
I don't have a pedal on mine either, but find I can get a bit of variable control by setting the downslope a bit longer then releasing the torch trigger and pressing it again as the current reduces (before the arc stops).
Basically if the weld pool starts to get away I release the trigger, then back on again. The longer you wait before hitting the trigger again the more the current reduces.
If you time it right its a bit like a manual pulse mode!
Steve
-
14th Aug 2019, 09:57 AM #11Most Valued Member
- Join Date
- Aug 2009
- Location
- Sydney, NSW, Australia
- Posts
- 1,844
Steve i think it does and thats a neat little trick i'll see how i go
-
14th Aug 2019, 10:36 PM #12Most Valued Member
- Join Date
- Sep 2010
- Location
- Lebrina
- Posts
- 1,915
I think you need to pay more attention to the shape of your infill patch. It is too flat (not enough curve) and once machined you will potentially have a thin spot. It would also be a good idea to ensure all of the joint is bevelled out to allow penetration.
What happened to the pieces that broke out originally? Often they are the best infill.
Is your little lathe up to the task of holding and machining the casting back to shape once welded?
Pay attention to the details as you will probably only get one go at this, two if you are really lucky.
-
15th Aug 2019, 09:15 AM #13Most Valued Member
- Join Date
- Aug 2009
- Location
- Sydney, NSW, Australia
- Posts
- 1,844
Hey Karl, The bits that had broken off were tiny pieces it wasn't one big piece i will attach a pic, i was going to use a die grinder bit in a drill to shape it doesn't have to be perfect and it doesn't have to be super strong as one of the internal ring gears is plastic
-
15th Aug 2019, 02:22 PM #14Most Valued Member
- Join Date
- Aug 2009
- Location
- Sydney, NSW, Australia
- Posts
- 1,844
Fighting with the tools tig regulator hose was one size regulator nipple was 1/4" solenoid nipple was 3/8" tried to make a hose fit but the hose kept folding in on its self than the solenoid wasnt working so pulled out the Unimig 200 Razor and just mig welded it
really good penetration but a bit of impurities not sure if it was because i had no backing and it was sucking air thru the gaps or if it were in the metal or my cleaning
after some sanding it came up pretty good
-
15th Aug 2019, 04:29 PM #15Most Valued Member
- Join Date
- Nov 2017
- Location
- Geelong, Australia
- Age
- 57
- Posts
- 2,673
Well done!!
Steve
Similar Threads
-
Work bench surface prep
By Commander_Keen in forum METALWORK GENERALReplies: 9Last Post: 10th Apr 2020, 04:26 PM -
Joint prep for stick welding skid plates
By Bryan in forum WELDINGReplies: 17Last Post: 1st Aug 2017, 11:59 PM -
Prep Work for welding Gal Steel
By capt'ngrumpy in forum WELDINGReplies: 9Last Post: 4th Feb 2013, 12:59 AM -
Implications of poor prep
By Legion in forum WELDINGReplies: 9Last Post: 26th Aug 2012, 06:37 AM -
The hole is too big
By neksmerj in forum METALWORK GENERALReplies: 15Last Post: 21st Jul 2007, 10:29 PM