Quote Originally Posted by MigOrTig View Post
Hi there!
I am asking this question for my father in law. He has a Unimig Razor 200 Tig. When he bought it he was given a manual that gave all the settings for particular metals. .....
I have this machine, it came with a Jasic branded operator's manual. There are three tables of welding settings:
Welding current vs electrode diameter for steel using MMA (stick).
Parameters for TIG welding titanium.
Parameters for TIG welding stainless steel.

If these are the tables you after let me know and I'll post photos here. There is no table for mild steel TIG.