Hi guys, thanks for the comments.
After laying down a couple of rods the electrode lead was cool, including where I repaired it (which was by cutting back to clean wire, soldering the full thickness, packing out with hotmelt glue and then heatshrinking), so that's good. The earth lead was slightly warm, about skin temperature, along the whole lead. I guess a larger lead would be beneficial but as this is the factory-installed lead, I don't think it's the cause of my current problem.
I was running the welder on a 25m 15a extension lead connected to a dedicated outlet in the meter box. However connecting the welder directly to the meter box outlet didn't change anything (which is consistent with other welders I've had over the years having run fine on the 15a extension lead). I also measured the voltage coming into the welder and it was a little over 240v which seems fine, though I'm not able to measure it under load.
So I think it comes down to somthing about the welder, either the electronics or the transformer. If I feel brave (or stupid) enough I could bypass the electronic current control and connect the power input directly to the transformer and see how that performs.
By the way, great work on tracing the circuit PlotJ! I actually contacted Cigweld to try to get a manual for this welder and they referred me to Cutting And Welding Support Site which is a great site with old Cigweld manuals and service information (incidentally including a circuit diagram for this machine!). Good pointers in parts availability.
-
3rd Mar 2021, 04:27 PM #17New Member
- Join Date
- Feb 2021
- Location
- Geelong, Australia
- Posts
- 4
Well I connected the power directly to the transformer and seemed to get slightly more welding power, but nothing like the 25 amps extra I'm looking for. I also took off the earth clamp and clamped the cable directly to an area of the work that I ground back, so earth is not an issue. I guess this will have to remain an unsolved problem.
I'm still keen to hear what setting any other users of this particular welder run 3.2mm 6013 rods on though.
-
3rd Mar 2021, 05:09 PM #18Most Valued Member
- Join Date
- Sep 2010
- Location
- Lebrina
- Posts
- 1,915
It's going back a bit now, but I did spend an hour or two on an Easywelder. As I recall, a 3.2 6013 electrode took every bit of power that they could muster. When those machines came out, the welding equipment world was full of machinery specs that told porkies. I don't believe those machines were ever capable of sustaining 140A outputs and would have rated them more like the 115-120A that you are experiencing. Their slightly smaller brother, the Compact 2 was allegedly 109A on the 3.2 setting and having owned one, I can confidently tell you that they would not run 3.2 electrodes for love nor money. We ran ours with 2.5's on the 3.2 setting with good results.
-
4th Mar 2021, 07:58 AM #19New Member
- Join Date
- Feb 2021
- Location
- Geelong, Australia
- Posts
- 4
Thanks Karl, that's very helpful info.
Similar Threads
-
PDF Manual available for CIGWELD Brumby 180 MIG Welder
By woodworkPete in forum WELDINGReplies: 5Last Post: 14th Apr 2020, 07:23 PM -
Manual for EMF/CIG Cigweld Transtig 250 Tig Welder AC/DC HF
By argeng in forum WELDINGReplies: 1Last Post: 20th Jul 2013, 09:25 AM -
Info on cheap Mig Welder
By Auskart in forum METALWORK GENERALReplies: 3Last Post: 14th Feb 2013, 11:18 PM -
CIGWELD MIG 200 Welder Or MAGMATE Pro 200
By Metal Head in forum WELDINGReplies: 1Last Post: 30th Sep 2008, 11:51 PM -
OTC TIG Welder Info
By nexusone in forum WELDINGReplies: 5Last Post: 11th Mar 2007, 09:48 AM