First time posting over the dark side
I picked up a jointer yesterday for a great price. But there's always a downside to something good that's cheap. As per the picture below the front of the fence there is two full thickness cracks as highlighted. The thickness that needs to be repaired is about 20mm and someone has attempted to do some sort of tack weld in the past. The fence still works okay however it's difficult to get a good lock on it.
Is anyone up for giving this a go for me? Can it be done? More than happy to pay what it's worth to repair. If you need anymore details or a better photo please don't hesitate to PM or post here. I live in Plenty (near Greensborough) and don't really want to stray too far to have it fixed.
Thanks in advance.
-Scott
-
18th Sep 2013, 12:12 AM #2
Its quite fixable only if you don't let someone who does not know what their doing near it.
Do not stick weld but go for braze welding. It will need to be ground out in a vee prep and Braze welded with Maganese bronze filler rod- not Tobin bronze but only with Maganese bronze filler . The casting is a bit complex and not well suited to the distortion that an inexperienced cast iron stick welder could place on it.
Grahame
-
18th Sep 2013, 12:34 AM #3Senior Member
- Join Date
- Jan 2010
- Location
- Bundoora, Melbourne.
- Posts
- 212
-
18th Sep 2013, 01:33 AM #4Most Valued Member
- Join Date
- May 2011
- Location
- Murray Bridge S Aust.
- Age
- 71
- Posts
- 5,959
Hi Scott, if you can't get it repaired, I have one that looks the same that I'm prepared to sell and swap for the broken one, as I can repair it myself.
My unit is a Woodman 4" jointer, I think they are all the same but sold under different brand names.
Regards
Kryn
-
18th Sep 2013, 12:33 PM #5Senior Member
- Join Date
- Jan 2010
- Location
- Bundoora, Melbourne.
- Posts
- 212
-
18th Sep 2013, 12:57 PM #6Member: Blue and white apron brigade
- Join Date
- Feb 2006
- Location
- Perth
- Posts
- 7,189
Scott, I can't see the back of that piece but assuming it is not a complex shape if necessary it looks like it could be remade with a piece of mild steel.
-
18th Sep 2013, 01:42 PM #7Senior Member
- Join Date
- Jan 2010
- Location
- Bundoora, Melbourne.
- Posts
- 212
Similar Threads
-
Cast iron pot repair
By lordnelson in forum METALWORK GENERALReplies: 19Last Post: 12th Oct 2011, 08:36 PM -
Cast iron table repair
By neksmerj in forum METALWORK GENERALReplies: 14Last Post: 22nd Jun 2011, 07:18 PM -
Cast iron repair for table saw arbor arm
By kman-oz in forum WELDINGReplies: 4Last Post: 27th Jul 2010, 02:11 PM -
Cast Iron Weld Repair
By Woodlee in forum WELDINGReplies: 4Last Post: 22nd Jun 2008, 10:13 PM -
Repair of Broken Cast Iron
By Grahame Collins in forum METALWORK GENERALReplies: 0Last Post: 11th Feb 2006, 11:35 PM