4th Oct 2009, 07:51 PM #1Member
- Join Date
- Oct 2003
- Location
- melbourne
- Age
- 67
- Posts
- 75
repair saw blade weld?
I send some Lucas blades to Shoda Travers (with specs) to be retipped besides the teeth falling off and making the blade too small they ground the outside of the blade for some reason. Well the teeth now come off often and they are hard to solder on because there isn't enough blade to hold them on the gig.
Can the blade be built up with weld? Would need to be hard I was thinking tool steel electrodes.
-
5th Oct 2009, 06:17 PM #2Novice
- Join Date
- Feb 2004
- Location
- kuranda north qld
- Posts
- 18
Mate its too late but i always send the blades back to the company that made them . one local fix it doctor ??? or whateverxxxxxxx made my blades cut soooooo bad i havent been game to try anyone else . bob
-
5th Oct 2009, 09:01 PM #3Member
- Join Date
- Oct 2003
- Location
- melbourne
- Age
- 67
- Posts
- 75
After mine were stuffed up I sent them back to Ace who made them and they rang me and asked who ground the blade at the back of the teeth? And what do you want us to do?
I asked if they could build it up with weld he repiied no blades are not mild steel and weld would be too soft.
THats why I'm asking here to see if harder electrodes would repair the damage.
-
5th Oct 2009, 10:41 PM #4China
- Join Date
- Dec 2005
- Location
- South Australia
- Posts
- 1,656
In could be done, but then you would have to re-grind the blade and then harden the blade, so for the price it would not be practical
-
6th Oct 2009, 06:12 PM #5Novice
- Join Date
- Feb 2004
- Location
- kuranda north qld
- Posts
- 18
i guess you ask the experts and follow their advice . or find a better expert!!! Looks like you got bad workmanship . try consumer affairs if you have the time ! cheers Bob
Similar Threads
-
Bubble at end of TIG weld
By Pete F in forum WELDINGReplies: 7Last Post: 2nd Sep 2009, 07:46 PM -
Rate my weld please!! :)
By dickies_ in forum WELDINGReplies: 5Last Post: 27th Jun 2009, 06:24 PM -
How do I weld Cast???
By g_man in forum WELDINGReplies: 27Last Post: 4th May 2009, 01:17 PM -
Cast Iron Weld Repair
By Woodlee in forum WELDINGReplies: 4Last Post: 22nd Jun 2008, 10:13 PM -
How do i weld a galvanised water tank(to repair)
By cilkorules in forum WELDINGReplies: 6Last Post: 28th Aug 2007, 08:46 PM