Which Grinding Wheel For Grinding Tungsten Electrodes
Hi,
I just used the search facility to find an answer to my question but was surprised not to find one!!
When I have ground my electrodes previously (at places of work) there has always been a green silicone carbide wheel to use. However, now I am finally getting around to setting up my TIG welder for action at home, I will need to buy the appropriate grinding wheel(s) to grind my electrodes.
So does one need a "GREEN" coloured silicone carbide wheel as I have previously encountered? If so, why is that? Will I also need to purchase an industrial diamond as a wheel dresser?
All advice would be appreciated.
Cheers
MH
-
2nd Aug 2009, 10:59 PM #2Senior Member
- Join Date
- May 2009
- Location
- SW Sydney
- Posts
- 101
Just use your regular grinder stones, your most likely not doing stuff that has to pass x-ray examinations so the small amount of contamination that may occur shouldn't bother you.
-
3rd Aug 2009, 11:43 AM #3Member
- Join Date
- Dec 2008
- Location
- Sydney
- Age
- 51
- Posts
- 84
According to the TAFE TIG course I'm in:
Grind with a diamond wheel. The hardest wheels you can find due to the hardness of the tungsten. And not too coarse either because tungsten tends to chip off rather than cut. Linisher afterwards helps to smooth it out. You don't want a bit of loose tungsten melting and falling off into the weld.
Dedicated wheel to avoid contamination.
-
3rd Aug 2009, 11:55 AM #4New Member
- Join Date
- Jul 2009
- Location
- melbourne
- Posts
- 2
Hi MH,
I've never really liked using grinding stones for some reason. Have you thought about just using a 4" or 5" sander? Thats what I mostly do at home. Otherwise you could set up a small linishing belt on your bench grinder - that'd be my preferred option. Sorry to waste your time by not actually answering your questions though!
Cheers
-
3rd Aug 2009, 07:24 PM #5
Chemical sharpening paste
An alternate to a grinder wheel is a chemical sharpening paste which works by you heating your tungsten red hot and dipping the tungsten in and out the material
It is an oxididant and erodes/burns /away metal to form a long tapered point.It is compeltely safe unless you eat it I suppose.
Its round the $20mark and cheaper than a dedicated wheel.It lasts for years. It takes a bit of hunting through the welding supply mobs but is still available.
Grahame
-
3rd Aug 2009, 09:52 PM #6Intermediate Member
- Join Date
- Jul 2009
- Location
- Bayswater Nth Melbourne
- Posts
- 32
G'day Grahame, after reading your earlier comment on the paste I got work to get some. Cost $40, When I asked why I was told "Courier costs". Any way, have you any tips when using it as it seamed to eat alot of the electrode and it didnt take the contaminate away very well. I've gone back to grinding for the moment but am feeling guitly about waisting the boss's money.
Regards, Col.
-
4th Aug 2009, 11:32 AM #7
G day Col
The paste was never designed for "removal" of contaminants ,solely as a sharpener.
Contamination is best avoided by a throrough cleaning of the work area and by careful manipulation of the torch and not "oops" accidentally dipping into the molten pool or touching the tungsten with the filler wire.
I get around it by rough grinding to remove the crap on the tungsten and then chemical prepping the tungsten.
It can be difficult to keep them to a 2 to 3 Diameter taper.
Its best achieved by keeping the dips into the paste shallow.
Re the $40 I had local quotes of $17 to $25. It may be time to look at a different supplier of welding consumables.
Generally if they know you and you buy a fair bit they should look after you.
Grahame
-
6th Aug 2009, 04:43 PM #8Senior Member
- Join Date
- Feb 2006
- Location
- Melbourne
- Age
- 65
- Posts
- 316
Hi,
Thanks to all those you replied with whatever advice you gave. I was intrigued by Grahame's advice about the paste. However, I have worked in the aircraft and ship industries and I never came across that idea - I'm not implying that it doesn't work but given Col's experience I am unlikely to go down that path - no offence Grahame.
Edster - You make a very good case regards a diamond wheel but won't it get clogged over time and liable to contaminate the electrode which is one of the things one wants to avoid? The green wheels I have always used have been of a fine nature and supposedly dedicated to grinding tungsten electrodes only. This was true in my time in the RAF when one workshop welder got into trouble for cleaning up a mild steel rod on it.
Bespoke Dude - I have seen people use linishing machines for grinding electrodes but they have also been used for other materials. I don't know if they are really ideal for this purpose.
However, I am interested to know why GREEN silicon carbide wheels are advised generally for this purpose.
Cheers
MH
-
6th Aug 2009, 07:18 PM #9
Its a bit of piddling around to grind the contaminants away IMHO .
Mostly operators seem to grip the tungsten between 2 sets of pliers and snap off the offending piece.
Then heatup and back into the paste.
The tungstens arent that dear $2.50 each or near that.
Its dropping the torch and cracking the ceramic that makes me cry.
Grahame
-
6th Aug 2009, 09:11 PM #10Member
- Join Date
- Dec 2008
- Location
- Sydney
- Age
- 51
- Posts
- 84
Metal Head - as mentioned, tungsten tends to chip off in large chips rather than get smoothed away with particles clogging the wheel. Nevertheless you aren't meant to sharpen tungsten on the wheel if it's got a lot of contaminants on it.
Nothing's wrong with the green silcon carbide. That definitely is a tougher wheel as well and the type we have at TAFE right now.
-
6th Aug 2009, 10:14 PM #11
I use a stone that I aquired that was a diahatsu diesel , ( were talking marine diesel engines here ) stone for regrinding stelite exhaust valve seats, it is worn past the diam needed for the engine exhaust valve seats 5" diam approx but set up in an old skill drill (3,000 rpm ) on a mandrel with the drill clamped to the bench it does a great job
So the advice is try a marine repair workshop or engineering workshop for wheels suitable for stellite exhaust valve seats .Ashore
The trouble with life is there's no background music.
-
7th Aug 2009, 03:21 PM #12Senior Member
- Join Date
- Feb 2006
- Location
- Melbourne
- Age
- 65
- Posts
- 316
-
7th Aug 2009, 03:24 PM #13Senior Member
- Join Date
- Feb 2006
- Location
- Melbourne
- Age
- 65
- Posts
- 316
Thanks also to Edstar & Ashmore for your additional comments. I will inquire about stellite wheels - I have never heard of them.
-
7th Aug 2009, 04:52 PM #14Most Valued Member
- Join Date
- Jun 2007
- Location
- sydney ( st marys )
- Age
- 64
- Posts
- 4,890
They were not reffering to Stellite wheels,but the wheels for grinding Stellite.
-
8th Aug 2009, 02:23 PM #15Senior Member
- Join Date
- Feb 2006
- Location
- Melbourne
- Age
- 65
- Posts
- 316
Similar Threads
-
Grinding wheel supplier?
By Greg Q in forum METALWORK GENERALReplies: 11Last Post: 23rd Jun 2008, 02:56 PM -
Lap grinding wheel
By ROB NZ in forum METALWORK GENERALReplies: 6Last Post: 20th Jan 2008, 06:42 AM