Hi everyone,

By now many of us who have the Tecmen brand helmets may have used up the clear plastic cover lens and spare.

Trying to source a replacement lens was a PITA as the potential candidates at the local welding supply were too big ,too small, too thick and too expensive.

I took my old cover lens to a plastics dealer,in my case Consolidated Plastics in Mackay.They were able to provide a sheet of poycarbonate exactly the same thickness as the original Tecmen lens.

For $5 I was able to purchase a sheet which provided 12 replacement lenses.

Hopefully you may have the same success with your local plastics dealer..

Grahame

Com_VC
1st Sep 2007, 06:30 PM
I ended up just using standard cig lenses and made up a rubber strip about 6mm or so to fill the missing space.