nigelpearson
29th Oct 2021, 07:07 AM
Took some rusty old 1/8" plate steel and cut into squares:
394626
Machined a rough die in the Hercus:
394625 394631
Got an assistant to stoke the coals:
394627 394628 394629
(actually BBQ heat beads, and he was just holding a hair dryer to push some air thru)
and after some bashing, got some dome shaped steel cups:
394630
A little grinding to take the corners off:
394633
and throw them in a bucket to try and get some rust overnight.
Day 2. Improve the forge a little:
394634
and create some extra patina, by re-heating, and bashing into concrete driveway with ball-pein:
394635
(original sample is on the left)
I'm half way there for this part of the job. Still have to weld little nail shafts on the back of the cup.
Still have to get my makeshift forge running hotter :((
Still have to work out how to do the other shapes :?
nigelpearson
31st Oct 2021, 01:47 PM
Got a MIG working, and welded some nails on the back:
394655
So that is the simplest 15 of the 200 total nails. This week I will try Propane-ing the forge, to get the steel beyond red.
nigelpearson
5th Nov 2021, 02:46 AM
Grabbed an old expansion burner my Dad used 30 years ago,
that I'm surprised they still seem to make/sell:
394686
and put it in my little forge. It makes a hell of a noise - sounds like a small combat jet?
https://photos.app.goo.gl/QBBKZtT6TBQFvQUEA
This thing is quite long, so I had to extend the "fire box" up:
394687
Now, this gets the steel slugs orange hot, but with 400mm of blue flame shooting straight up, this is a bit of a challenge to get the slugs safely resting there. So I weld some slats in the top tube, and try some BBQ rocks:
394688
Big mistake.
The packet the rocks came in said "Lava rock may contain gas and may explode when heated, ejecting particles for several meters." Yeah, right, I thought. Just needless safety B.S., I thought.
Nope. Fired it up, and the rocks pop and spit and crack and chunks go flying off. Not good.
Another trip to Bunnings, and buy some ceramic thingies. Factory neighbour convinces me to heat from the top (because all the heat is just going straight up in the air with my big burner), so we try his propane burner and a fire brick:
394689
I didn't like this setup. The flame bounces around in there and out in all directions. Including towards my face. Result is still only orange hot after a few minutes, and to get slugs out I have to put burner aside, then reach in there with pliers and fish around. Seems slower and loses a little bit of vital heat.
After leaving that to cool down, I go back to my tall fire box idea (after fitting a mesh grill with larger holes):
394690
This seems easier to use, as I can more easily position slugs under the edges of the ceramics for more or less heat, but bashing slugs into the die is also not going as well as I would like.
I get then out of the fire box and into the die, then pick up a hammer and bash away, but they are not getting the nice curve from the face of the die, or expanding out on the back. Even if I heat and bash a few times, and try a cold chisel (long centre punch) in the back:
394691
Get through a dozen or so, and then neighbour comes to assist. Proposes some casting. Throws a large ladle on the heat, and tried pouring a few cc of Aluminium in the die before I shove a nail in the molten metal. We try a few, but it is very hard to pour just a little metal from a large spoon/cup. Either a lot of metal pours over the side, or a lot stays on the top of the die.
394692
They are a good shape, but cleaning the waste off the back as well as then having to age them to look like rusty steel, will not be manageable. Another dead end.
So, I'm giving up on blacksmithing for now.
A better anvil might have helped, but bashing slugs into a little die is just losing too much heat.