View Full Version : CNC Lathe
NGrimberg
13th Apr 2020, 06:04 PM
What are some ways to reduce chatter when boring out a deep hole on a Lathe?
pipeclay
13th Apr 2020, 06:32 PM
Increase or decrease feed rate.
Increase or decrease surface speed.
Use the largest boring bar.
Reduce the nose radius of the tip.
snapatap
15th Apr 2020, 06:23 PM
buy a Sandvik anti-vibe boring bar
BaronJ
11th May 2020, 06:55 PM
buy a Sandvik anti-vibe boring bar
It would be cheaper to wrap some plumbers solder wire around the bar.
rcaffin
12th May 2020, 09:04 PM
It would be cheaper to wrap some plumbers solder wire around the bar.
Or use some sheet lead and some (thin) BluTack. Yes, that does work.