I made myself a Hammer and tong rack. All hand tool work no electricity involved.
Lots of punching, sliding, & drifting.
https://uploads.tapatalk-cdn.com/20191011/10d8d4b7dd13a0001b2cb69bc6b1ed13.jpghttps://uploads.tapatalk-cdn.com/20191011/f7f9f34b822020d86a0bf0b4f84a52e8.jpg
The base rail started life as a 20x40mm bar. Both ends were upset to 20x80mm to form the shouldered tenon. This took me a day & a half!
https://uploads.tapatalk-cdn.com/20191011/8275c4b84d7b9f81f0ac89be3374b118.jpg
https://uploads.tapatalk-cdn.com/20191011/afc17a8a675960958a1e8c2b29c4ff5a.jpg
https://uploads.tapatalk-cdn.com/20191011/0f5d3500fde5cb0fbd80b0bf65c3e01a.jpghttps://uploads.tapatalk-cdn.com/20191011/b8f8219eeebbac2f96d0b74bee01824a.jpg
The slot in the legs starts parallel with the bar and is turned 90 deg. This was an interesting process.
https://uploads.tapatalk-cdn.com/20191011/47bd4bce27acb7f63e243823d7ceccd1.jpg
All operations were done under careful supervision and it was made sure there were no interruptions.
https://uploads.tapatalk-cdn.com/20191011/680a72e4277b4211cfe5fdf704a8ac04.jpg
Lots of punching, sliding, & drifting.
https://uploads.tapatalk-cdn.com/20191011/10d8d4b7dd13a0001b2cb69bc6b1ed13.jpghttps://uploads.tapatalk-cdn.com/20191011/f7f9f34b822020d86a0bf0b4f84a52e8.jpg
The base rail started life as a 20x40mm bar. Both ends were upset to 20x80mm to form the shouldered tenon. This took me a day & a half!
https://uploads.tapatalk-cdn.com/20191011/8275c4b84d7b9f81f0ac89be3374b118.jpg
https://uploads.tapatalk-cdn.com/20191011/afc17a8a675960958a1e8c2b29c4ff5a.jpg
https://uploads.tapatalk-cdn.com/20191011/0f5d3500fde5cb0fbd80b0bf65c3e01a.jpghttps://uploads.tapatalk-cdn.com/20191011/b8f8219eeebbac2f96d0b74bee01824a.jpg
The slot in the legs starts parallel with the bar and is turned 90 deg. This was an interesting process.
https://uploads.tapatalk-cdn.com/20191011/47bd4bce27acb7f63e243823d7ceccd1.jpg
All operations were done under careful supervision and it was made sure there were no interruptions.
https://uploads.tapatalk-cdn.com/20191011/680a72e4277b4211cfe5fdf704a8ac04.jpg