View Full Version : Who has an oxy cutting torch ?
Grahame Collins
9th Aug 2005, 07:49 PM
Who has an oxy cutting torch ?
Next hard question is "Who can use it their oxy torch properly?".
Any takers for a run through for the basics on gas axemanship ?
Or would a write up on gmaw be preferred -thats MIG if you did not know.
I thought it might busy up the board a little bit.It's getting a bit sleepy around here.
Comment please !
Grahame
Greolt
9th Aug 2005, 08:02 PM
Going by your exellent series on stick welding I think that would be a great idea.
Not so much for me (I am a boilermaker) but many would find something like that very informative.
So I reckon go your hardest:)
Greolt
boban
9th Aug 2005, 09:21 PM
Comment please !
Grahame
I've got one and have cut with it but to be honest, beginner would be too nice for my oxy cutting skills. I did some research and saw the pictures of the lovely cuts but I'll be stuffed if I can get that to happen over more than 50mm. And they are never straight.
That said my mig welding is good. I found preparation to be the key.
Seriously interested in hearing from a pro, so go for it mate.
Optimark
9th Aug 2005, 09:31 PM
I have an oxy cuting kit, in fact I have a complete Comet 3 kit I purchased second hand 23 years ago. It was bought off a tradie who had to replace it on a building site as it had the Mickey Mouse gauges, the site required the new vertical gauge for him to stay on site.
I have cut a few things and have to say that when cutting a ½" plate of steel for a bench top I was making (and still have) I learnt on the job so to speak. I did last year, watch a tradesman doing a cut on ½" sheet steel and thought of how neat and precise the cut was made.
At times I have made spectacular cuts, but the next one wasn't that crash hot, so I'm obviously lacking on just what it is I need to do.
Any lessons you can offer would be received gratefully.
Mick.
Stuart
9th Aug 2005, 10:52 PM
Plasma cutting Mmmmmmmmmmm
Ashore
9th Aug 2005, 11:48 PM
I have a gas axe have used one for 90% of my at sea life, still but rearly use it these days but still keep a full gas set at home. Have cut most stuff even stainless, though wet electrodes do a better job , Hardened container mounts , most thickness steel from 1/8th to 6" bar .
For basic cutting close all valves on the gun, open valve on gun and set pressure at bottle for acetylene at about 90-100 kpa close valve on gun. open rear oxy valve almost fully depress cutter trigger and set oxy pressure at bottle 300-400 kpa at bottle leave rear valve open
Open acetylene and light , open front oxy and adjust till just blue flame , no yellow and flame touches the tip , depress lever ( trigger) ensure flame does not go out or lift away from tip , adjust rear valve to suit and if necessary front valve.
Hold flame on edge of job and wait till small sparks jump from heated surface , as this usually indicates that the material is hot enough to cut , depress lever , main flame just above surface and bring down to touch and start cutting in a slow fluid motion , ensure you are cutting the materrial , speed of cut comes with practise the thicker the material the slower the cut
Always have enough oxy to blow slag away without cooling the job too much
Increase pressure for very thick work
Keep all the holes on your tip clean of slag etc
Use right size tip for material your cutting
All the rest is practise or being taught hands on
And always turn gas off at bottles and release pressure from lines
Buy fit and use anti flash back arrestors at the gun
Check , inspect hoses and o'rings regularly Leaking perferated hoses will kill you , and can be replaced for bugger all.
Don't fit new fittings to hoses unless you are trained and have the correct tools
Never use grease oil on fittings or threads
Store bottles in free air space , been a few vechicles blown up by leaking bottles left overnight
When you burn yourself , and you will , cool the burnt area in ice etc for at least 20 minutes as the sub surface fats in your skin will still boil
Hope this helps
Russell
Useless infomation for the day
Man who run behind car get exhausted.
graemet
10th Aug 2005, 10:45 PM
I've had a CIG colt22 oxy set for 30 years and use the cutter very rarely as it uses loads of oxy and with my poor technique, the cuts take more time to clean up than cutting with a friction disc. I use the oxy cutter for really heavy stuff that doesn't need to look pretty. Any tips would be appreciated.
Cheers,
Graeme
DanP
11th Aug 2005, 05:31 PM
The best tip I can give - you need to get a set of tip cleaners and use them. Nothing stuffs a cut like a dirty tip.
Next best tip. Always acetylene first. Open it first, shut it off first.
Dan
Mulga
12th Aug 2005, 10:06 PM
Be a good idea for a topic. Very useful to some I think.
Still use the oxy for Silver and Brass soldering, not so much for cutting anymore, although when we were making points
(before customers could buy them less retail) the oxy and forge were indespensible.
The Plasma we now have use at work and on "foriegners" will handle up to 75mm so why reinvent the wheel on that one.
Always been a firm believer in learn everything about a tool even if you don't use it for that purpose.
Mulga
Grahame Collins
18th Aug 2005, 11:46 PM
Ashore has done a fine job with the basics of Oxy cutting. I can add a few things that I have observed over the years of teaching students.
Safety
Never take the oxy plant for granted. Even the smallest set of CYLINDERS mistreated have the potential to kill should things go wrong. Thermally,acetylene is the most efficient gas known to man. It has the greatest explosive range as well.
It ranges between 3 % acetylene to 97 air mix and 92 % acetylene to 8% air mix.
If you want experience how a diesel engine combustion sequence works, just leave a trace of oil or grease on the regulator thread where it screws into the cylinder. The bad news is that after the 2000 Lbs. cylinder pressure hits the grease or oil, an explosion usually follows. On the large cylinders it means the regulator explodes at just about face level.
Setting up
.Always make sure fittings are the correct ones for the plant. If you are a scrooge don’t skimp here. I would caution people not to mix differening brands of OXY gear particularly the Comet 3 clones. The tolerances differ and you put yourself at risk. In my humble opinion the CIG Comet 3 rates with the best the world has to offer.
New operators tend to set the torch flame too high. At the neutral flame setting if you have to raise you voice to be heard clearly over the noise of the flame its set too high.
You do not need trainer wheels for any cut under 300mm long. If you are really hard up to cut a straight line setup an angle section with a handle . 50mm equal angle is ok.Cut 8mm from the top to give a vertical height of 42 mm. If I remember it measures 42 from plate surface to the shoulder formed by the nut against the cutting nozzle. This is for a type 41 cutting nozzle only . You might have to check this measurement as after 20 years my memory is a bit hazy.
That’s enough for starters I will have to finish this latter.
Grahame
Grahame Collins
20th Aug 2005, 09:28 PM
Before lighting your cutting torch for the first time in a session you are wise to check a few things first. Over the years I have got into a habit of doing a quick visual check over the connections followed by running my hands almost folded in a loose fist dragged over hoses and connections to check physically for gas leaks.
I always check my cutting nozzle for cleanliness and if not satisfied clean it with the correct diameter cleaning wire.
The tip here is to start with one obviously too large and use the one that fits as you work your way down. Incorrect undersize cleaning wires do damage to cutting nozzles by elongating the hole opening and destroying the shape of the jet of gas emitted. Dirty or damaged nozzles will not cut well.
A word here about nozzle sizes. Cutting Nozzle jet holes are measured in millimetres and parts thereof. Designated sizes of 6, 8, 12 and 15 translate to .6mm, .8mm 1.2mm and 1.5mm. -.6mm will cut down to 3mm and 1.5mm will cut to 75mm thick steel.
Steel is heated to an ignition point by the preheater flame and a jet of pure oxygen is directed at the preheated point. The result is that the steel ignites or burns.
My comments here apply to a Comet 3 cutting head but most others are similar. Open the torch primary oxygen valve all of the way. This is the one closest to the hose. It supplies both the cutting stream oxygen and that for the pre heat flame.
Open the acetylene valve about a third of a full turn and light the flame.
The acetylene flame should be adjusted until the oily smoke dissipates and the flame becomes very bright. It should lift slightly off the nozzle opening. At this time gently open the oxygen pre heater valve closest to the nozzle. Your flame will form the neutral shape which is a number of cones which do the preheating.
Adjustment of the preheater valve so that the cones form a soft rounded shape at the nozzle, will produce the ideal neutral setting required for cutting. The nozzle is held with a millimetre or two of gap under the flame tips. Heat the plate edge until it becomes an orange colour and fully depress the lever. A correct cutting speed will result in a stream of slag inclining in the direction of the cut accompanied by a tearing, ripping noise occurring on plates 10mm and up.
To be continued
Grahame
BobL
5th Oct 2007, 10:05 PM
Last time I used an oxy to cut steel was back in high school maybe 40 years ago?
Last week I used an oxy to cut the hook out for this (http://www.woodworkforums.ubeaut.com.au/showthread.php?t=57904) tool but my efforts at cutting were . . . let's call them . . . "slow and erratic"!. Yesterday I did a search on the forum here and found up this thread and WHALA! - this evening I applied the refreshed knowledge and . . . . . hot knife through butter time :D what a satisfying spray of hot metal and sparks - nearly as good as chainsaw milling!
Thanks Graeme and Ashore :2tsup:
Cheers
DJ’s Timber
5th Oct 2007, 10:25 PM
Funny that you should bring this up Bob, yesterday and today I have been cutting secondhand steel for the newly acquired hopper for the mill and also had to put some 25mm holes in the base plates which are 20mm thick for the columns and one off the boys said to me "how do you get such a neat hole with no slag and no gunk" and I replied "clean tip, correct adjustment and lots of practice" with a grin on my face.
Good to know that I can still wield a gas axe with good precision :2tsup: :U.
China
5th Oct 2007, 10:38 PM
Optimark , interesting point about the vertical gauges 5 years ago I was told by CIG the I had to replace my vertical gauges with the micky mouse type as they could not handle the presure in the latest cylinders
NewLou
5th Oct 2007, 11:15 PM
Gidday:D
I got to admit one of my fav metal working processes at the moment is OXY! I love the dam thing and am in awe of those able to wield a flame blade effectively! I particularly love flame gouging!
Love setting up a piece of mild steel stock and cutting it with a beautiful smooth finish on the 'quickie' (Our automatic OXY setup at trade school!) I can cut competently by hand but am far from being able to get that smooth finish at right angles that I'd love to be able to achieve consistently!
Anywaz for those of you that are familiar with the Woodrat Joinery system the creators of this gem have created a hand operated aluminum extrusion that enables x-y axis movement (from right to left or left to right) n I reckon I could fabricate a gem of a semi automatic oxy cutting rig using the rat as a basis...................... Will start posting a few PICS once I start toying with ideas!
REgards Lou:D
thesupervisor
5th Oct 2007, 11:33 PM
i use lpg due to the cost i always seem to have lots of slag is this due to the lpg?
i think lpg is only 200 or 300 degrees cooler than acet
Snap-on
6th Oct 2007, 11:30 AM
Let's see some pics of people cutting stainless etc with a oxy/acet/iron powder torch.... he he he
Cliff Rogers
6th Oct 2007, 12:06 PM
Let's see some pics of people cutting stainless etc with a oxy/acet/iron powder torch.... he he he
You first. :2tsup:
Grahame Collins
6th Oct 2007, 01:08 PM
Let's see some pics of people cutting stainless etc with a oxy/acet/iron powder torch.... he he he
The cutting hardware has all to one to the junkyard many moons ago my friend. Pictures are all you have left. I tried to find an illustration in my text books in vain.
Why bother if you can now get a cheaper ,faster and cleaner plasma. Oxy acetylene/lpg has its place but not in this particular circumstance.
Even I have been dragged kicking and screaming into the modern age.
Grahame
Grahame Collins
6th Oct 2007, 01:17 PM
Let's see some pics of people cutting stainless etc with a oxy/acet/iron powder torch.... he he he
The cutting hardware has all to one to the junkyard many moons ago my friend. Pictures are all you have left. I tried to find an illustration in my text books in vain.
Why bother if you can now get a cheaper ,faster and cleaner plasma. Oxy acetylene/lpg has its place but not in this particular circumstance.
Even I have been dragged kicking and screaming into the modern age.
Grahame
journeyman Mick
6th Oct 2007, 03:39 PM
Before lighting your cutting torch for the first time in a session you are wise to check a few things first. Over the years I have got into a habit of doing a quick visual check over the connections followed by running my hands almost folded in a loose fist dragged over hoses and connections to check physically for gas leaks.
I always check my cutting nozzle for cleanliness and if not satisfied clean it with the correct diameter cleaning wire.
The tip here is to start with one obviously too large and use the one that fits as you work your way down. Incorrect undersize cleaning wires do damage to cutting nozzles by elongating the hole opening and destroying the shape of the jet of gas emitted. Dirty or damaged nozzles will not cut well.
A word here about nozzle sizes. Cutting Nozzle jet holes are measured in millimetres and parts thereof. Designated sizes of 6, 8, 12 and 15 translate to .6mm, .8mm 1.2mm and 1.5mm. -.6mm will cut down to 3mm and 1.5mm will cut to 75mm thick steel.
Steel is heated to an ignition point by the preheater flame and a jet of pure oxygen is directed at the preheated point. The result is that the steel ignites or burns.
My comments here apply to a Comet 3 cutting head but most others are similar. Open the torch primary oxygen valve all of the way. This is the one closest to the hose. It supplies both the cutting stream oxygen and that for the pre heat flame.
Open the acetylene valve about a third of a full turn and light the flame.
The acetylene flame should be adjusted until the oily smoke dissipates and the flame becomes very bright. It should lift slightly off the nozzle opening. At this time gently open the oxygen pre heater valve closest to the nozzle. Your flame will form the neutral shape which is a number of cones which do the preheating.
Adjustment of the preheater valve so that the cones form a soft rounded shape at the nozzle, will produce the ideal neutral setting required for cutting. The nozzle is held with a millimetre or two of gap under the flame tips. Heat the plate edge until it becomes an orange colour and fully depress the lever. A correct cutting speed will result in a stream of slag inclining in the direction of the cut accompanied by a tearing, ripping noise occurring on plates 10mm and up.
To be continued
Grahame
Grahame,
I know this thread is a few years old now, but any chance of posting some more info?
Mick
Grahame Collins
6th Oct 2007, 06:33 PM
Mick,
What are you looking for specifically? Rather than be too general it much better to specify on what you wish to acheive,or if anybody who wants to make a post.
Grahame
journeyman Mick
6th Oct 2007, 09:38 PM
Grahame,
not exactly sure, but I spotted the post and noticed the "to be continued" without any further posts from you.:D Perhaps gas pressures would be helpful, plus a trouble shooting guide, ie if it looks like this you're doing this wrong etc.
Mick
fenderbelly
6th Oct 2007, 10:25 PM
if you're cutting thick plate warming the underside first, makes a big difference.
If you have trouble getting started when cutting round bar, hold a thin piece of scrap to the side and you will find you can start you're cut much easier.
and the most important thing is to hold the torch firmly,don't try to strangle it as this will only make your hands shake, relax it aint gonna bite.
Grahame Collins
7th Oct 2007, 11:42 AM
noticed the "to be continued" without any further posts from you.:D Perhaps gas pressures would be helpful, plus a trouble shooting guide, ie if it looks like this you're doing this wrong etc.
Mick
Gday Mick
A fresh thread is posted.
I have been playing around trying to do a photographic thing, but the cant' get pics right at the flame.I don'tseem to have the right equipment.
I would appreciate if any photographic tecchy type could clearly photograph the hand held torch head showing a macro shot neutral flame flame with the blue cones just above the plate surface.
I have searched and Googled big time and can't find any illustrations to suit the power points
Grahame:doh:
Fossil
7th Oct 2007, 01:13 PM
My camera is at work, but I'll bring it home on Tuesday and do it, if no one else can do it sooner. :)
antoni
7th Oct 2007, 01:14 PM
Hi all ok who's got one of the Henrob 2000 torch (kits ) are they as go as they say ?
Thanks Tony
Grahame Collins
7th Oct 2007, 04:21 PM
Hi all ok who's got one of the Henrob 2000 torch (kits ) are they as go as they say ?
Thanks Tony
Tony,
We purchased one for school thinking that it would be easier for the students. Our experience is that the low pressure regulators required for effective use were extras.
The vendors did not give support one could normally expect.The did not follow up on phone calls or emails very well at all and generally did not seem to be supportive of a customer who had spent a good deal of money with them.
We had trouble matching thesupplied American Gas thread to to Australian code regulator. Our p/time teachers assistant whose other job is as a licensed repair man for Oxy Acetylene regulators and torches.
Had it not been for him we would have not got the unit operating at all.
Yes it will weld aluminium and so forth,but honestly A Tig does the job better.
Four years down the track we are back to using the normal cutting torch and $600 wasted sits unused at the rear of a storeroom.
Thats is our experience others may have fared better.The unit does not seem to be vigorously marketed here as I don't see mention of it too often.
Grahame
China
7th Oct 2007, 04:33 PM
Ditto!
BobL
7th Oct 2007, 06:35 PM
My BIL talks about a trick he does where he heats up the edge of plate and then pushes the oxygen cutting jet and starts cutting then he turns of the acetylene and keeps cutting - he says if you do it smoothly and slowly enough it will keep cutting! Apparently the heat of the burning metal is enough to keep heating the metal ahead of it - kind of like a metal firestorm!
BobL
7th Oct 2007, 06:42 PM
Gday Mick
A fresh thread is posted.
I have been playing around trying to do a photographic thing, but the cant' get pics right at the flame.I don'tseem to have the right equipment.
I would appreciate if any photographic tecchy type could clearly photograph the hand held torch head showing a macro shot neutral flame flame with the blue cones just above the plate surface.
:
A camera with a point or spot exposure meter that will expose for the exact point on the flame you wish to see is what you need. Most consumer digitals will perform some kind of average exposure across the image and the sensor simply cannot handle the dynamic range of an oxy flame. A digital SLR camera with a macro/telephoto should be able to do this I would have a crack although I am very nervous about exposing mine to such an environment. If no one else does it I will ask the photo techy guys at work - they love this sort of thing - photography, sparks, noise etc.
Cheers
Wood Butcher
7th Oct 2007, 07:27 PM
My BIL talks about a trick he does where he heats up the edge of plate and then pushes the oxygen cutting jet and starts cutting then he turns of the acetylene and keeps cutting - he says if you do it smoothly and slowly enough it will keep cutting! Apparently the heat of the burning metal is enough to keep heating the metal ahead of it - kind of like a metal firestorm!I've done this. Bloody hard to get everything just right but a real good trick to do when showing Yr 11 students Oxy Cutting.:p
Fossil
18th Oct 2007, 11:55 AM
My camera is at work, but I'll bring it home on Tuesday and do it, if no one else can do it sooner. :)
Well I am not as smart as I thought!
I have tried to take clear pics with my camera, but I can't seem to get it right. I was using a happy snappy camera from work, as my MIL bent the card interface pins on my digi slr. If someone will foot the $425.00 bill for the camera repair, I can take the pics and send them to Graham. Any takers????? :-
Ashore
18th Oct 2007, 02:58 PM
I've done this. Bloody hard to get everything just right but a real good trick to do when showing Yr 11 students Oxy Cutting.:p
Yep always good for a demo, its like using an oxy lance, now thats an experiance :U
Powered by vBulletin® Version 4.2.5 Copyright © 2024 vBulletin Solutions Inc. All rights reserved.