DSEL74
16th Apr 2017, 12:15 PM
I started building a new eye bender on Monday unfortunately unforeseen unfortunate events have & will prevent me from finishing for a while.
Adjustment pin holes for the clamping bar. 1/2" drilled on the Denbigh. Drilled 2up back to back combined thickness 20mm
https://uploads.tapatalk-cdn.com/20170416/0e3a786009a02f05453e350fed95e88f.jpg
Mock assembly
https://uploads.tapatalk-cdn.com/20170416/ca49d8cfaffb0e201caf9f263b8b6f96.jpg
1" SHS to be bolted to the base so it can be held in the vice. My previous one had angle iron but some of the old post vices are too worn to hold well on such a thin section.
https://uploads.tapatalk-cdn.com/20170416/d6cd79d4ddc6072956c14a882111be4b.jpg
Drilling the main arm for the die pins.
https://uploads.tapatalk-cdn.com/20170416/09232f11c26e8ebd12f2b4d17b90842f.jpg
I timed the actual drill time, set up and alignment not included. It takes the Denbigh 4:31.28 minutes to put a through hole in. So if you add up all those holes and multiply by 4 1/2 min it takes a while.
https://uploads.tapatalk-cdn.com/20170416/b2ab660b7c9010890713b60ff71a094e.jpg
Adjustment pin holes for the clamping bar. 1/2" drilled on the Denbigh. Drilled 2up back to back combined thickness 20mm
https://uploads.tapatalk-cdn.com/20170416/0e3a786009a02f05453e350fed95e88f.jpg
Mock assembly
https://uploads.tapatalk-cdn.com/20170416/ca49d8cfaffb0e201caf9f263b8b6f96.jpg
1" SHS to be bolted to the base so it can be held in the vice. My previous one had angle iron but some of the old post vices are too worn to hold well on such a thin section.
https://uploads.tapatalk-cdn.com/20170416/d6cd79d4ddc6072956c14a882111be4b.jpg
Drilling the main arm for the die pins.
https://uploads.tapatalk-cdn.com/20170416/09232f11c26e8ebd12f2b4d17b90842f.jpg
I timed the actual drill time, set up and alignment not included. It takes the Denbigh 4:31.28 minutes to put a through hole in. So if you add up all those holes and multiply by 4 1/2 min it takes a while.
https://uploads.tapatalk-cdn.com/20170416/b2ab660b7c9010890713b60ff71a094e.jpg